Medium intermediate frequency furnaces are widely used for the smelting of non-ferrous metals and ferrous metals. Compared with other casting and smelting equipment, they have the advantages of short smelting time, less alloy element burnout, accurate control of the temperature and composition of molten metal, and less environmental pollution. However, the medium intermediate frequency furnace generally has the problem of short lining service life during use, especially when smelting different types of alloys or when the melting temperature of the alloy is high, the medium frequency induction furnace is more susceptible to damage. This article uses the process of knotting the lining with different vibrators to explore the impact of different furnace building methods on the furnace age, so as to reduce the factory production cost.

01 The impact of power on the life of the lining
After sintering, the lining will form a three-layer structure, the sintering layer close to the charge position, the transition layer in the middle, and the loose layer close to the furnace wall. With the increase of smelting furnaces, the sintering layer gradually increases. When the power is too large, the strong stirring force generated by electromagnetic induction causes the molten iron to form a large impact force on the lining. In addition, if the electric furnace is operated at high power for a long time, the local temperature of the furnace lining will be too high. When the charge density is too low, the charge is easy to be suspended in the middle of the furnace body. If the charge is not rammed in time, there is a risk of bridging accidents. When the power is too small, the smelting time is extended, affecting production efficiency. And in continuous smelting, keeping some molten iron at the bottom of each electric furnace has a certain effect on shortening the smelting time, improving smelting efficiency, and increasing the life of the furnace lining.
02 The impact of the charge addition method on the life of the furnace lining
The charging method has a certain degree of influence on the life of the furnace lining. When performing the charging operation, the principle of adding the charge with a low melting point first and the charge with a high melting point later should be followed. The recarburizer should be added when there is at least 1/3 of the molten iron in the electric furnace to avoid adding it to the bottom of the electric furnace. Practice shows that when a large amount of recarburizer is added to the bottom of the furnace for daily smelting operations, the bottom of the furnace body will be severely eroded. At the same time, the cleanliness of the charge should be ensured as much as possible, and the use of seals or aluminum alloy castings is strictly prohibited.
03 The impact of smelting operation on the life of the intermediate frequency furnace lining
Correct smelting operation has an important impact on improving the service life of the furnace lining. During intermittent operation, the temperature of the furnace lining will go through a periodic cycle from low temperature to high temperature to low temperature, repeatedly heating and cooling the furnace lining, and the linear shrinkage rate of the sintered layer of the furnace lining close to the charge will increase, and the furnace lining is prone to cracks, especially when it is below 800℃, which will reduce the life of the furnace lining. During continuous smelting, the furnace temperature changes little and is basically maintained above 800℃. The linear shrinkage rate of the sintered layer of the furnace lining becomes smaller, and the life of the furnace lining is improved.
FAQ
Why is the particle size distribution of furnace lining materials crucial to the lifespan of an induction furnace?
A: A reasonable particle size distribution significantly improves the packing density of the furnace lining. Too much fine powder, while resulting in faster sintering, leads to greater shrinkage and a higher risk of through-cracks; too many large particles result in a less dense lining, allowing molten steel to easily penetrate the gaps. High-quality furnace lining material should optimize the ratio of coarse, medium, and fine particles to ensure a dense structure during furnace construction, effectively resisting the mechanical erosion and chemical attack of molten steel.
How do the “binding strength” and “sintering process” during furnace construction affect the later furnace life?
A: Uneven furnace construction (binding) is a major cause of premature localized lining detachment or furnace leakage.
Binding: Uniform binding strength must be ensured. Insufficient strength leads to low density, while excessive strength may cause delamination (poor interlayer bonding).
Sintering: The key lies in the baking temperature rise profile. Strict low-temperature, long-time baking must be implemented to remove bound water and structural water. If the temperature rises too quickly, the high pressure from moisture evaporation can cause microcracks to form inside the furnace lining. These microcracks will rapidly expand during subsequent high-temperature melting.
How does the “slag basicity” during the melting process erode the lining of an induction furnace?
A: Induction furnaces typically select the slag system based on the lining properties (acidic/basic/neutral).
If an acidic lining (such as quartz) is used, adding too much high-basicity slag (such as high-calcium slag) will cause a violent chemical reaction, resulting in the formation of low-melting-point compounds on the lining surface, leading to rapid melting and erosion.
Technicians must strictly control the chemical composition of the slag to match the lining material and promptly reduce “elephant trunk-shaped” erosion near the liquid level through slag removal operations.