5 factors of graphite electrode consumption for heating furnace and holding furnace

The electrode is the last part of the short power supply network of heating furnace and holding furnace. A strong arc is generated at the end of the graphite electrode to melt the charge and heat the slag. That is, the electrode is the central hub for converting electrical energy into thermal energy. When the electrode is working, it is subject to high temperature, furnace gas oxidation and collapse impact. Especially the connection between the two electrodes has a larger resistance and lower conductivity than other places. It is easy to trip, oxidize, fall off and break, which causes great consumption of the electrode, prolongs the smelting time and reduces productivity.

graphite electrode
graphite electrode

The consumption of graphite electrodes comes from the following 5 factors: oxidation, sublimation, dissolution, peeling and breaking

Oxidation – graphite electrodes

When the temperature exceeds 400℃, oxygen can penetrate into the graphite surface for oxidation. When the temperature exceeds 550℃~600℃, oxidation intensifies. The oxidation rate is sensitive to the oxygen concentration and airflow velocity near the electrode. Under normal operation of the electric furnace, the oxidation consumption rate accounts for about 50%-60% of the total pure consumption (except for the breakage consumption), which is mainly affected by the high temperature airflow.

Sublimation

Graphite is easy to sublimate at high temperature. Under normal operation, the sublimation consumption rate can reach 40% of the total electrode consumption (excluding the breakage consumption). Excessive current will lead to increased sublimation consumption. Measures to reduce electrode sublimation consumption: avoid excessive use of strong current.

Melting

Graphite is easy to melt in liquid slag, so short arc operation or immersion operation will cause increased electrode consumption. When the slag layer is thick, the electrode end and the slag liquid are in contact and partially melted.

Peeling – graphite electrodes

Electrode peeling is caused by thermal strain caused by temperature difference. During production operation, the electrode end is often locally at high temperature, resulting in thermal bending and peeling.

Generally, excessive strong current and short arc operation will cause electrode peeling. Therefore, to reduce electrode peeling consumption, long arc is better than short arc.

Breakage

Electrode breakage usually occurs at the highest joint or joint seat of the electrode column. The reasons for electrode breakage are as follows:

The furnace cover is not in the correct position and the electrode hole is not centered;

Failure or accident of the electrode lifting system;

Mixed use of products from different manufacturers;Measures to reduce electrode breakage:

Keep the furnace cover in the correct position and confirm that the electrode hole is centered before power is supplied each time;

Do a good job of equipment maintenance to ensure the normal operation of the electrode lifting system and reduce accidents;

Use the electrode correctly and strengthen electrode maintenance.

Usually, the electric furnace may encounter about 10 electrode breakages per month, accounting for 10% of the total electrode consumption. If the broken electrode is recycled and used, the consumption ratio is reduced to 3%.

Summary

After analysis, it can be seen that in the heating furnace and insulation furnace for the production of slag wool, graphite electrode oxidation is the main factor. In addition, after an investigation of the slag wool production line of a certain iron plant in Shandong, it was found that the appearance of the electrode has changed greatly during the heat adjustment process alone, so long-life electrodes are becoming more and more important to slag wool plants and steel plants.

When examining the adaptability of long-life electrodes to holding furnaces, the physical and chemical properties of the materials, such as mechanical properties, electrothermal properties, electrical conductivity, and oxidation resistance, as well as the matching accuracy of the electrodes and joints, the reliability of the connections, and the length of the adaptable equipment (the up and down travel of the electrodes), should be analyzed one by one. In addition, the power transmission mode, operation method, and process of the equipment should be understood and mastered as necessary.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time