Cracks in castable

After a period of operation, the boiler will have wear on the lining. In severe cases, the boiler may even be directly damaged, affecting normal operation. In order to extend the service life of the boiler, castables are basically used to repair the parts of the boiler that are more severely worn, but after the construction is completed, castable may crack. Why does this problem occur? To solve this problem, you must first know the cause of the cracks.

Control of water-cement ratio during castable mixing

Adding too much water to the castable during mixing can easily make the internal porosity of the castable high after molding, reduce the strength, and take too long to solidify naturally, which will increase the curing time. If too little water is added, the castable will have poor fluidity, vibration is not dense, and it is easy to leave pores and bubbles, and the strength will be greatly reduced.

Mixing time and construction time control

When mixing the castable, the mixing time must be strictly controlled. If the time is too short, the castable will be unevenly mixed, not dense, and the strength will be reduced; if the mixing time is too long, the castable is prone to stratification, fine powder floats on the surface, and aggregate sinks to the bottom, resulting in reduced strength and easy peeling of the castable. The castable should be used up within 30 minutes after mixing.

Poor demoulding time control

Here, demoulding is performed before the castable is completely hardened. When is the most appropriate time to demould? The castables should be removed only when the strength of the castable can be guaranteed and its edges and corners are not damaged by demoulding. To facilitate demoulding, a layer of engine oil should be applied to the casting surface of all molds before pouring.

Castables curing time control

After the construction of the castable is completed, there should be enough natural drying period so that most of the moisture in the refractory layer can be precipitated, in order to prevent a large amount of moisture from not being discharged in time during the furnace baking, causing the refractory layer to burst and fall off. The principle of furnace baking is “should be long rather than short, slow rather than fast”. The drying process should be carried out according to the pre-established drying curve. The heating speed should be uniform and stable, and the constant temperature time and temperature should be well controlled to keep the temperature fluctuation within ±20℃. It should be prevented from heating up too fast, and the moisture cannot be discharged in time, breaking through the wear-resistant and refractory layer; secondly, it should be prevented from excessive temperature fluctuation in the refractory and wear-resistant layer, which will generate huge thermal stress and cause the wear-resistant and refractory layer to crack, bulge, and fall off.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information