Analysis of Common Erosion and Damage Mechanisms in Ladle and Tundish Sliding Nozzles

Sliding nozzles refractory materials, also known as sliding plates, are key components of continuous casting flow control systems. Sliding plate bricks are a key component of the sliding nozzles, directly controlling the molten steel and determining its functionality. The manufacturing process for sliding plates differs from that of previous refractory materials. They function both as a molten steel injection device and as a flow regulator. In addition to mixing, forming, firing, and inspection, brick manufacturing also involves machining, assembly, and overall external adjustment of the sliding surface.

During operation, sliding nozzles are subjected to extremely demanding conditions, as they must withstand prolonged chemical and physical erosion from high-temperature molten steel, intense and transient thermal shock, and mechanical wear. Furthermore, to ensure smooth opening and closing of the steel flow, the sliding surface flatness and dimensions must meet stringent requirements. Therefore, sliding plates must exhibit strong resistance to erosion and erosion from molten steel and slag, high high-temperature strength and wear resistance, and good thermal shock and oxidation resistance. Currently, the vast majority of ladles and tundishes, both domestically and internationally, are equipped with sliding nozzle systems. The sliding gate system consists of a sliding mechanism, an upper gate, a sliding plate, and a lower gate. The sliding plates are divided into upper and lower plates, and their shape depends on the required geometry of the mechanism. Upper and lower plates with the same dimensions can be used interchangeably, but plates with different dimensions cannot be used interchangeably.

Mechanism of Slide Plate Erosion

01 Thermomechanical Corrosion

Thermomechanical corrosion first occurs during the use of the slide plates. The slide plates are at a very low temperature before use. During pouring, the inner hole of the slide plates suddenly comes into contact with the hot molten steel (1600°C), causing intense thermal shock (temperature fluctuation of approximately 1400°C). This generates tensile stress outside the casting hole that exceeds the strength of the slide plates, leading to the formation of radiating microcracks centered on the casting hole. The formation of cracks facilitates the diffusion, accumulation, and penetration of foreign impurities, further accelerating chemical corrosion. Simultaneously, chemical corrosion reactions further promote the formation and propagation of cracks, leading to the gradual enlargement and destruction of the slide plate casting hole. Furthermore, the erosion of hot molten steel damages the refractory material in the areas of friction with the steel, causing spalling and chipping.

02 Thermochemical erosion

Thermochemical erosion is another major cause of slide plate damage. During use, the refractory materials used in slide plates come into contact with high-temperature molten steel and slag, causing a series of chemical reactions and chemical erosion. According to the different chemical damage mechanisms of different steel grades to slide plates, Baosteel’s current steel grades can be divided into three categories, namely, killed steel, high-oxygen high-manganese steel, and calcium-treated steel. According to different usage conditions, slide plates of corresponding materials are selected, which can increase the service life of the slide plates and reduce the cost of refractory materials. Chemical mechanism of damage to Al2O3-C and ZrO2-Al2O3-C slide plates: (1) Carbon oxidation: There are two main ways for graphite and carbon to oxidize: one is that the oxygen in the molten steel, especially the high-oxygen steel, oxidizes carbon to form pores, and then iron penetrates the pores and causes the molten steel to adhere to the surface of the slide plate; the other is that the oxygen in the air oxidizes carbon and molten steel to form low-melting products, which then continue to erode and penetrate along the pores. (2) Decomposition of mullite: Mullite decomposes to varying degrees after use, transforming into columnar and crystalline corundum crystals, forming a porous structure, destroying the original dense eutectic structure composed of mullite and clinoptilolite, making the structure loose, the organization deteriorating, and the strength and corrosion resistance greatly reduced, accelerating the damage of the slide. (3) Corrosion of the slide by (Mn) and (Fe): SiO2 in the slide reacts with FeO and MnO in the steel and slag to form low-melting-point mineral phases 2FeO·SiO2 (1205℃) and MnO·SiO2 (1291℃). (4) Damage to the slide by (Ca): Al2O3·SiO2 reacts with CaO in the steel and slag to form low-melting-point 2CaO·Al2O3·SiO2 (1327℃) and 12CaO·7Al2O3 (1392℃).

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information