There are various types of furnace linings used in electric furnaces for producing ferroalloys. The type of lining used for different ferroalloys is determined by the melting temperature of the ferroalloy, the acidity or alkalinity of the slag, and the type of electric furnace. Generally, acidic slag is used for producing high-carbon ferromanganese, ferromanganese-silicon alloys, and low-carbon ferromanganese-silicon alloys, and carbon linings are typically used; alkaline slag is used for producing high-carbon ferrochrome, and magnesia linings are typically used; ferrosilicon and ferrosilicon-chromium alloys, due to their high temperatures, also generally use carbon linings; while refining furnaces and alkaline slag are used for producing medium- and low-carbon ferromanganese and ferrochrome, and magnesia rammed-material linings are typically used.
A certain ferroalloy company has mainly focused on producing ferromanganese-silicon alloys in recent years. During the production process, furnace lining damage frequently occurs. Therefore, the damage mechanism of carbon linings used in the production of ferromanganese-silicon alloys was analyzed. Carbonaceous furnace linings used in the production of ferromanganese alloys can be classified into carbon block linings and cold-rammed paste linings based on the shape of the raw materials used; and into insulated linings and water-cooled linings based on their thermal insulation performance. Regardless of the shape of the raw materials or the thermal insulation performance, they are essentially furnace linings constructed from carbonaceous materials.
A new furnace lining, with proper use and maintenance, can have a lifespan of over ten years; however, with poor use and maintenance, its lifespan can be less than a year or even just a few months. Therefore, understanding the causes of furnace lining damage is crucial.
Causes of Furnace Lining Damage
Inappropriate Furnace Drying Procedures
In a certain region, newly built manganese-silicon alloy submerged arc furnaces with a capacity of 30 MVA or higher experienced furnace bottom burn-through accidents within a year of commissioning (some even within two months). During furnace cleaning and maintenance, it was discovered that the carbon bricks below the electrodes had almost stood upright, and the area beneath the carbon bricks was filled with manganese-silicon alloy. The cause of this alloy seeping into the lower layer of the carbon bricks puzzled and perplexed the company’s technical personnel.
Commonly used furnace lining materials include not only carbonaceous materials but also clay bricks, high-alumina bricks, refractory granules, asbestos boards, filler paste, and binders. These materials all contain a certain amount of moisture, and the filler paste and binders contain a large amount of volatile matter. If prebaked carbon bricks are used, they contain even more volatile substances. Both water and volatile substances will turn into gases and be released when exposed to high temperatures.
An inappropriate furnace drying procedure when a new furnace lining is first put into use can cause lining damage. Shortening the furnace drying time will cause the temperature to rise too quickly. When the furnace temperature rises too rapidly, a large amount of moisture and volatile gases from the newly laid carbon bricks and related materials will be rapidly released, and the energy released at this time is also very large. If this energy is not released slowly and sufficiently, it will cause the carbon bricks at the bottom of the furnace to loosen, and a large number of vent holes will appear between the carbon bricks in the furnace lining. Liquid manganese silicon alloy will seep into the furnace lining through these vent holes, arching the carbon bricks at the bottom of the furnace, causing a certain degree of damage to the furnace bottom, and even leading to a furnace bottom leakage accident.
These newly built manganese silicon alloy submerged arc furnaces with a capacity of 30MVA or more all use furnace linings built with prebaked carbon bricks. Therefore, an unreasonable furnace drying system is one of the reasons for furnace bottom leakage. At that time, two new electric furnaces did not experience furnace leakage accidents when they were put into operation because the equipment was constantly malfunctioning during power supply, and was in a state of stop-and-go operation. This provided sufficient time for the release of water vapor and volatiles in the furnace, and by sheer coincidence, the furnace lining was preserved.
Unreasonable Electricity Usage System
Since the transformer’s capacity is determined at the factory, the basic operating cost of the transformer borne by the manufacturing enterprise is fixed.
(1) Overload operation can achieve good economic benefits. If more electricity is consumed during production, the basic operating cost per kilowatt-hour will decrease, that is, the price of electricity per kilowatt-hour will decrease, so the electricity cost per ton of alloy product will decrease. With fixed parameters, the size of the electric furnace is also fixed. In this case, an increase in the amount of electricity input into the furnace raises the furnace temperature, speeds up the melting process, and increases the output. In recent years, in order to obtain higher output and better economic benefits, electric furnaces have generally been operating under overload conditions, with overloads ranging from 10% to 20% to 30% to 40%.
(2) Overload operation can cause damage to the furnace lining. Although overload operation brings great economic benefits to enterprises, excessive overload also causes great damage to the furnace lining. Overload is basically achieved by first exceeding the voltage and then the current. Excessive current requires deep electrode insertion. When the desired current cannot be achieved, the electrode must be released prematurely. If the electrode extension is not properly controlled, the working end of the electrode will become too long, damaging the furnace bottom. Currently, no refractory material can withstand the temperature of the electrode arc. Over time, the carbon bricks below the electrode base are prone to floating, damaging the top layer of carbon bricks.
Long-term water leakage inside the furnace
Water leakage inside the furnace is extremely dangerous for smelting production. When the equipment leaks severely, the electric furnace cannot operate at full capacity, easily causing large-scale material collapse and endangering the safety of on-site operators. Furthermore, the evaporation and decomposition of leaking water require a large amount of heat, resulting in heat loss within the furnace and increased alloy power consumption.
If liquid water encounters high temperatures, it will rapidly decompose into hydrogen and oxygen. When hot carbon bricks encounter oxygen, oxidation is very rapid, potentially causing a furnace leak. If the furnace wall is soaked with water, the water will vaporize at high temperatures, causing the furnace wall to expand rapidly. If the water cannot be removed in time, it will cause damage to the furnace wall.
Poor furnace shell welding leads to air leakage.
Carbon furnace linings are neither acidic nor basic, therefore they are resistant to both acidic and basic slag corrosion. They also have high refractoriness and a high load softening temperature, so under normal circumstances, the high temperatures generated during smelting (not the high temperatures of arcing), erosion, and the acidity or alkalinity of the slag have little impact. From these aspects, carbon furnace linings are relatively ideal for ferroalloy smelting. However, their fatal weakness is their extremely poor high-temperature oxidation resistance.
If the furnace shell welding is poor, or if the welds crack over time, the carbon furnace lining will inevitably be exposed to air. During production, the temperature of the carbon bricks in the furnace wall can reach over 300℃, providing conditions for the carbon furnace lining to react with oxygen. The lining will rapidly oxidize to produce carbon dioxide, leading to corrosion and damage.
Practice has shown that the oxidation of the furnace lining by oxygen begins in the gaps between the carbon bricks and then spreads to both sides. The oxidized areas are relatively smooth, without obvious sharp edges, and can develop in depth. When repairing a leaking furnace, first clean the burned-through area, then seal it with electrode paste or plugging mud, ensuring that the welded joints of the furnace shell are airtight.
Damage to Furnace Lining by Heavy Metals
The main raw material for the production of silicon manganese alloy is manganese ore, which is generally associated with heavy metals, primarily lead, tin, and silver. Lead has a melting point of 327.5℃ and a specific gravity of 11.35 g/cm³; tin has a melting point of 231.89℃ and a specific gravity of 7.3 g/cm³; silver has a melting point of 962℃ and a specific gravity of 10.49 g/cm³. Siemens manganese alloy has a melting point of 1240–1300℃ and a specific gravity of 6.0–6.4 g/cm³. These heavy metals all have lower melting points and higher specific gravity than silicon manganese alloy. During high-temperature smelting, the lower-melting-point heavy metals are reduced before manganese and iron. Because these initially reduced heavy metals are heavier, they easily seep into the furnace lining through the brick seams, causing the bricks to arch and damaging the furnace lining.
Damage to the furnace lining due to lack of regular maintenance
Under normal circumstances, the furnace lining should be shut down for maintenance after about one year of use, especially at the taphole area, where prolonged exposure to high temperatures, erosion, and oxidation will cause more severe damage than other parts. If the electric arc furnace is operated for extended periods without regular maintenance, the damage to the furnace lining will inevitably worsen, potentially leading to a furnace lining leak.
Conclusion
This paper summarizes and analyzes the causes of damage to the furnace lining of manganese-silicon alloy electric arc furnaces. While these causes are not exhaustive, they are very common. The aim is to analyze these causes and find corresponding solutions to better extend the service life of the furnace lining. An extended furnace lining life will correspondingly increase productivity and reduce alloy costs.