From the time a blast furnace is completed and put into production to the end of a generation of furnace service, Blast furnace hearth and furnace bottom are always immersed in liquid slag iron, and are in a high-temperature and high-pressure smelting process for a long time. The erosion mechanism of the lining of the Blast furnace hearth and furnace bottom is very complex, with multiple factors acting at the same time, and these factors also interact and influence each other. The understanding of some erosion mechanisms has not yet been completely unified. Relatively consistent views can be roughly attributed to two categories, namely mechanical erosion and chemical erosion.

Mechanical erosion
01 Thermal stress
The hot surface of the hearth refractory material is in contact with liquid slag iron, and the temperature is usually higher than 1350℃, and the cooling water temperature of the cooling wall contacted by its cold surface is 25~45℃. It can be concluded that the radial temperature difference of the hearth is as high as about 1300℃, which will produce huge thermal stress. The hearth refractory material with a thickness of about 1 meter, under the combined action of high temperature, high pressure and ultra-large temperature difference, conducts heat transfer, and undergoes multiple physical and chemical actions, which may cause various damage phenomena such as thermal expansion and contraction, fracture, and crushing. The stress distribution in the furnace is very complex and belongs to the research content of interdisciplinary subjects. The current research is not comprehensive.
02 Mechanical scouring and friction
The inevitable circulation of molten iron and the rise and fall of the slag iron liquid level in the furnace will cause mechanical scouring and friction on the surface of the furnace lining refractory materials. The wear resistance of refractory materials in high pressure and high temperature environment for a long time will be significantly reduced, seriously affecting their service life; with the fluctuation of furnace conditions, the lining protective layer (slag skin) formed on the contact surface with slag iron will also fall off. Once it falls off, the furnace lining refractory materials will be directly subjected to the mechanical scouring and friction of the slag iron flow.
03 Static pressure and shear force
The density of liquid iron is about 7.6t/m³. The continuous melting of iron in the furnace and the iron stored in the dead iron layer weigh hundreds of tons. At the same time, the hot air pressure in large blast furnaces in China is very high. The above factors make the static pressure on the refractory materials at the bottom of the furnace higher. For carbon bricks located at the junction of the furnace and the bottom of the furnace, the above static pressure plays a shearing role. The compressive strength of carbon bricks is generally 20~40MPa at room temperature, while the flexural strength is only 7~15MPa at room temperature. The strength of refractory materials at high temperatures is lower than that at room temperature, and the pressure they bear is close to the gravity they bear, so they are easily crushed by pressure. Once the refractory materials are broken or cracked, the high-temperature and high-pressure liquid iron can easily invade the brick seams or refractory pores. As the molten iron invades the pores of the refractory materials, the contact surface between the molten iron and the refractory materials increases rapidly, and the carbonaceous particles will be surrounded by the molten iron, which accelerates their melting into the molten iron. This is the penetration erosion of the molten iron. In order to reduce the penetration and erosion of molten iron on the furnace, carbon bricks with high processing precision, microporous structure, high thermal conductivity and high resistance to molten iron dissolution should be used, and the size of brick joints during masonry should be strictly controlled.
04 Molten iron buoyancy
In addition to being subjected to great static pressure and shear force, the furnace refractory materials are also affected by the buoyancy of molten iron. The volume density of refractory materials is usually around 1.5~3.0t/m3, which is only a fraction of the density of molten iron. Refractory materials are easy to float on liquid molten iron. The bottom of the furnace is usually provided with a certain diameter near the furnace shell, and the extrusion and friction of the brick structure are relied on to prevent the refractory materials from floating up. Once this force exceeds the bearing range of the refractory materials used, it will cause the refractory materials to break and deform. As long as a certain part or a small part of the furnace is eroded, a large amount of refractory materials will float and be damaged due to the buoyancy of molten iron.
The above mechanical erosion forces affect each other and act together on the carbon bricks of the furnace, which has a great impact on the carbon bricks of the furnace.
Chemical erosion
01 Carburization erosion of molten iron
The carbon content of pig iron for steelmaking under modern production conditions is generally maintained between 4.5% and 5.4%, and it is not clear what the maximum can reach. The carbon content of pig iron is related to factors such as the volume of the blast furnace, the hot air pressure, and the smelting intensity. Pig iron is an unsaturated solution of carbon in an iron-carbon melt. Since there is always molten iron in the furnace, carburization reaction is always occurring in the furnace. Carbon in coke, coal powder, and carbon bricks can all undergo carburization reaction. Once the graphitized carbon bricks and semi-graphitized carbon bricks in carbon bricks come into contact with molten iron, they will quickly undergo carburization reaction, that is, the carbon bricks will quickly melt in the furnace.
02 Redox erosion
Many types of redox reactions can occur under the chemical conditions in the furnace, which is relatively complex. For example, the water-gas reaction caused by water leakage in cooling equipment such as tuyere will cause carbon bricks to oxidize and lose carbon, pulverize and produce cracks, and ultimately lead to a decrease in the strength of carbon bricks in the furnace. For example, the redox reaction of alkali metal elements such as potassium, sodium, lead, and zinc in the lower part of the blast furnace can generally cause the common loose belts or annular cracks in carbon bricks.
Mechanical erosion and chemical erosion act on the Blast furnace hearth and furnace bottom at the same time. It cannot be said which factor comes first and which comes later. The influence of various factors varies under different circumstances. With the continuous changes in production conditions, the physical and chemical environment in the Blast furnace hearth is also constantly changing. It can only be said that under certain specific conditions, some types of erosion are relatively strong, while others are relatively weak.