Application of castable prefabricated block ladle repair and maintenance technology

The technology of using aluminum-magnesium spinel castable prefabricated block to repair and maintain the ladle is as follows:

PART.01 Using ladle wall working layer digging and patching technology

During the first minor repair and cooling process of the ladle, due to the material of the refractory material, sometimes the 1st to 4th ring of the prefabricated block of the wall working layer will produce shrinkage joints of more than 10mm or abnormal melting loss. In order to ensure safe use, it is usually necessary to dismantle from the top of the wall working layer to the shrinkage joint or abnormal melting loss part, in which a large amount of available refractory materials will be removed, causing great waste, and requiring a lot of manpower and material resources.

By analyzing the refractory materials used in the ladle on site, under the premise that the overall condition of the ladle refractory materials is good, only the wall prefabricated block at the shrinkage joint or abnormal melting loss parts are removed by local digging and repairing, and then the actual size of the digging and repairing parts is measured, and the sample drawing is enlarged on site. After the refractory materials are processed accordingly, they are masonry-laid to the demolished part, and finally the door is closed with square bricks. The use of excavation and patching technology can avoid the waste of refractory materials caused by large-scale demolition of prefabricated block and save masonry workload.

prefabricated block

PART.02 Repair technology combining shaped refractory bricks with unshaped refractory materials

During the use of the ladle, some impurities in the molten steel erode the refractory materials of the ladle lining. Due to the different degrees of erosion, unevenness and melting and slag sticking will occur in the ladle wall working layer prefabricated block during use. In addition, the production process requires that the weight of a 300t ladle must be between 128t and 140t to produce grade steel, which makes it difficult to repair the ladle.

For ladle weights less than 128t during use, ladle that is too light must be repaired, otherwise it will affect the safety of the ladle. Previously, all the ladle wall corundum repair materials were used for large-scale patching. The life of the ladle and the empty ladle weight were maintained at normal levels. However, due to the high price of corundum repair materials and the large amount of materials used, the average life of the ladle wall working layer is low, and the residual thickness is thin and the effect is not good.

For local melting loss, after testing, it is believed that the use of special repair materials is more effective. In order to meet the requirements of ladle repair, the repair materials must have the following properties:

⑴ Good coating construction performance, that is, the material must have good adhesion to the base material. First, the developed repair material should be easy to apply and adhere to the repair surface, and secondly, it should not scatter or collapse when the coating repair material layer is thick.

⑵ It has both air hardness and thermal hardness. At the construction temperature of ladle coating (about 50-60℃), the coating material should be able to harden quickly for subsequent spraying. At the baking temperature, it can produce sufficient medium and low temperature strength to form a firm bond with the repair surface.

⑶ Good resistance to rapid baking and bursting.

⑷ Good high temperature volume stability, basically consistent with the volume stability of the ladle bottom or ladle wall material, so as to ensure that during the alternating use of the ladle, the repair material will not crack or even peel off due to the large difference in volume change with the base material, making the repair material ineffective.

⑸ Excellent slag resistance.

Through extensive use, it has been proved that this repair material has good high temperature resistance and corrosion resistance. It has the advantages of good fluidity, convenient construction, good adhesion to the original brick layer, and long service life when used locally. The test results on the working layer of the aluminum-magnesium carbon steel ladle wall show that most of this aluminum-magnesium repair material still remains in the repaired part after 15 furnaces, making the service life of the ladle relatively stable. However, it is difficult to repair large-area melt damage. Because it is an amorphous material, a large amount of use on the vertical surface makes the mutual support insufficient. In particular, to repair the melt damage surface of the ladle at a certain height, it is often necessary to wait for a section to be repaired and hardened before continuing to repair upwards. It is very time-consuming and labor-intensive, and the repair time is long, which affects the turnover speed of the ladle. Therefore, this repair method has limitations in use.

The wax stone brick patching method is another method to explore ladle repair. Although the wax stone brick has a low volume density, the melting loss of the prefabricated block in the working layer of the ladle wall and the slag sticking phenomenon of the prefabricated block in the working layer of the ladle wall will not cause the ladle to be overweight, but the wax stone bricks cannot meet the requirements of ensuring the use of the ladle for one cycle under the scouring of high-temperature molten steel. This method is not ideal among the ladle repair methods. High-aluminum bricks are patched in the later stage. The ladle is used until the residual thickness of the ladle wall is about 90 to 100 mm. When it enters the last minor repair, high-aluminum bricks are used to patch the serious melting loss areas. Because the ladle wall itself is too thin and has no mutual support, cracks are generated. As a supplementary means, this method has little practical significance. From the situation of unpacking after using this repair method, a large area of ​​cold steel has penetrated into the permanent layer. Moreover, after patching, the packaging operator is easily blinded by the appearance during the judgment process, and the potential danger is very large. This repair method is not desirable and has been eliminated. Mid-term patching of high aluminum: We tried to use high aluminum bricks to patch the working layer of the ladle wall when the residual thickness of the ladle wall was about 120-130mm. After half a year of practice, we think it is more suitable for use on 250t ladle. High aluminum patching bricks have the performance of high temperature molten steel erosion and corrosion resistance. The aluminum-magnesium-carbon bricks of the ladle wall have been melted after about 50 furnaces, and the weight has been reduced. At this time, patching will not cause the problem of overweight of the ladle. When the ladle is used for about 50 furnaces, the surface of the refractory material lining of the ladle is still uniformly melted. At this time, patching is more convenient to operate and the quality of patching is also better. During the trial, more than 10 ladles were repaired with this patching method, and a relatively ideal use effect was achieved, and it was fully promoted.

Determining the appropriate repair materials and modes not only improves the service life of the ladle, but also indirectly reduces the labor intensity of the workers, facilitates the operator to correctly judge the refractory materials of the ladle lining, the safe use of the ladle, and the normal turnover of the ladle in the steelmaking production process, achieving a relatively ideal effect. The use of reasonable and correct ladle repair methods has obvious effects on the role of ladle refractory materials in actual production applications, cost reduction and efficiency improvement, and accident reduction. It should be further explored and reasonably applied. Baosteel’s 300t ladle adopts a repair technology combining high-aluminum bricks and amorphous refractory materials. The specific operation method is to first remove the uneven surface residues and cold steel of the ladle wall, repair the parts with large melting loss, and then use the ladle wall repair material to apply a thickness of 10 to 20 mm on the surface of the pit, and then apply a layer of high-aluminum bricks on the repaired surface, 50 mm thick, and finally use the ladle wall repair material to repair a layer on the surface of the high-aluminum bricks and the joints at both ends. When selecting the cladding wall repair material and high-alumina brick, considering the matching between the refractory materials and whether other impurities will be introduced to affect the quality of the steel products, the main components of the selected cladding wall repair material and high-alumina brick are Al2O3 and MgO, which will not affect the quality of the steel products, so the cladding wall repair material and high-alumina brick are selected.

This repair method combined with the repair material and high-alumina brick can not only repair the cracks and gaps in the working layer in time, but also repair some parts that are not easy to repair. In this way, it can effectively prevent the weak cladding wall from continuing to melt and avoid the weak parts of the molten steel from continuing to erode, improve the safety factor of the ladle, and each minor repair of the ladle can achieve a stable service life.

prefabricated block

PART.03 Accurately determine the residual thickness of the prefabricated block of the offline ladle and determine the reasonable repair mode

After the ladle is offline, the repair mode must be determined first. In the past, the residual thickness of the prefabricated block was mainly determined by the operator based on work experience. There are large uncertainties and there may be misjudgments and wrong judgments. The repair plan is determined according to the data after the misjudgment and wrong judgment. There are quality risks caused by the ladle repair not being in place or the repair being too conservative, resulting in waste of refractory materials. Through careful observation of the offline ladle, it is found that there is a clear regularity in the change of the residual thickness of the working layer of the ladle wall. The wider the residual surface, the thinner the residual thickness. There is a certain proportional relationship between the residual surface width and the residual brick thickness. According to this fixed proportional relationship, after measuring the width of the refractory brick at the thinnest part of the entire prefabricated block, the thickness of the residual brick at that place can be accurately determined. In this way, accurate reference data can be provided for determining the repair mode of the ladle, eliminating the quality and safety risks of the ladle caused by human misjudgment and wrong judgment, and at the same time, it can also avoid the waste of refractory masonry.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information