Application of Magnesia Carbon Bricks in Steelmaking Electric Arc Furnaces and Their Damage Mechanism

The working environment of the electric furnace lining is very harsh, which is a considerable test for the lining refractory materials. The two most severe points are the temperature difference in the electric furnace and the change in the slag composition.

The operation of ordinary electric furnaces is to complete the three stages of melting, oxidation and reduction in the electric furnace. Among them, the operation of UHP electric furnaces is to use forced melting to greatly increase the melting speed, and alloying is achieved after refining in the LF furnace. Therefore, the specific power level of UHP electric furnaces is generally above 600kvA per 1t steel, and modern ones reach 1000kvA per 1t steel. Figure 1 shows the relationship between power level, electric furnace temperature and melting time.

Application of Magnesia Carbon Bricks in Steelmaking Electric Arc Furnaces and Their Damage Mechanism

The high power level of the UHP electric furnace makes the heat load on the surface of the furnace lining as high as 1000kvA/m2. The furnace lining is rarely shielded during the melting period. In addition, the highest radiation level forms the furnace hot spot on the masonry opposite the arc. The minimum heat load is between the phases, that is, the “cold zone”. The difference in heat load between the hot spot and the “cold zone” can reach 60%. It can be seen that the temperature in the electric furnace is spatially uneven. Under such conditions, the temperature of some hot spots may reach more than 2000℃, which is quite unfavorable to the slag resistance of magnesia carbon bricks. The slag breaks through these hot spots and then erodes the entire brick body. In addition, the temperature difference will cause the thermal stress inside the brick body to increase, and it is easy to peel off under the mechanical scouring of the slag.

Another feature of electric furnace steelmaking is the variety of steel types. The variety of steel grades brings about the changeable composition and properties of slag, which makes the slag erosion of the furnace wall MgO-C bricks very complicated. The strong boiling and stirring of molten steel-slag and the thermal shock of the arc make the furnace lining suffer more severe erosion than the converter: Therefore, when the service life of MgO-C bricks in large converters reaches thousands of furnaces, or even tens of thousands of furnaces (using the slag splashing furnace protection process), the life of the electric furnace wall is still only 300~500 furnaces. When smelting the slag of the same steel grade, the composition of the initial slag and the final slag will vary greatly due to the change of smelting parameters; when smelting the initial slag and final slag of different steel grades, the variation of their composition is more obvious. Similar to the situation of slag in the converter process, the most prominent variation is binary basicity.

The traditional electric furnace steelmaking process includes the entire melting-refining process. A furnace of steel lasts for 3~4 hours. The composition of the slag and the reduction slag in the oxidation period varies greatly. For the refractory materials of the furnace lining, they have to experience the alternating erosion of acidic to alkaline slag. For example, for 1Cr18Ni19Ti steel, the C/S of the initial slag is <1, while the final slag is >2. The phase combination and chemical composition changes of the molten pool slag and splashing slag in different smelting cycles of the traditional steelmaking process have been studied in detail using electron probes. Since the percentage of each phase has not been determined, the comprehensive composition of the slag cannot be estimated, but the composition variation of the entire slag can also be observed from the changes in the chemical composition of the phases. The melting period and oxidation period are oxidized slag; the refining period and alloy period are reduced slag. Except for some marker elements of special alloy steel, the phase combination rules of each phase in the slag are normal, but the crystallization behavior can be analyzed from the micro-region composition of its phase. For example, the banded structure and composition changes of spinel in the molten pool slag are caused by the changes in the slag composition during the smelting cycle; it also reflects the mutual replacement of cations in the spinel nucleation and growth process: from high chromium type to high aluminum type, which is also the characterization of the chromium return and deoxidation process. The spinel in the oxidation period is still high chromium type, while it becomes high FeOn type in the refining-alloying period.

The corrosion of magnesia carbon bricks is carried out under the alternation and circulation of various slag compositions. The corrosion behavior of the working surface of refractory bricks and magnesia carbon bricks changes in each furnace, each steelmaking, and even in different smelting stages of a steelmaking furnace. From the change of slag basicity to the change of slag oxidation, and even the change of slag fluidity in this process, these changes will have different effects on the corrosion of magnesia carbon bricks.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information