In high-temperature industrial applications, refractory castable precast blocks serve as a critical lining material for equipment such as kilns and blast furnaces. Their performance and stability directly impact the equipment’s operating efficiency and lifespan. However, in actual production, surface damage such as flaking, cracking, and pulverization often occurs, leading to increased equipment downtime and maintenance and increased production costs. This article analyzes the root causes of these damages from multiple perspectives, including materials, processes, and the environment, and proposes systematic solutions.
NO.01 Core Cause of Surface Damage: The Synergistic Effects of Materials, Processes, and the Environment
1. Material Selection and Preparation Process Defects
Insufficient raw material purity is the primary factor leading to surface damage. Excessive levels of alkali metal impurities such as sodium oxide and potassium oxide in low-quality refractory aggregates (such as uncalcined andalusite) react with carbon dioxide in the air to form carbonates, which cause volume expansion and cracking. For example, a steel company using alumina aggregate with an alkali content of 0.8% experienced a surface pulverization rate three times higher than that of high-quality aggregate (alkali content ≤0.3%). Improper particle grading can also weaken material properties. If the aggregate particle size is too large, increased cement is required to fill gaps, resulting in increased porosity. If the particle size is too small, the material strength is reduced. Experiments have shown that precast blocks with a continuous gradation (5-3mm:3-1mm:1-0mm = 4:3:3) have a 25% increase in flexural strength compared to a single gradation.
Uncontrolled sintering is another key issue. Excessively high sintering temperatures can lead to abnormal grain growth, resulting in a brittle structure; while temperatures that are too low can lead to incomplete sintering and excessive porosity. At one cement plant, a sintering temperature deviation of ±50°C increased the apparent porosity of precast blocks from 18% to 25%, and reduced wear resistance by 40%.
2. Chemical Attack and Atmosphere Effects
Alkaline atmosphere attack is particularly prevalent in the metallurgical and glass industries. Iron oxide and calcium oxide in the slag react with aluminum oxide in the castable to form low-melting-point phases (such as calcium aluminoferrite), resulting in a loose structure. For example, when the SO₂ gas concentration in a glass melting furnace reaches 50 ppm, the thickness of the carbonized layer on the surface of high-alumina cement castables increases by 2 mm per month.
Thermal stress cycles exacerbate material degradation. When an intermittent kiln is started and stopped, the temperature difference between the surface and interior of the precast blocks can reach 300°C, generating tensile stress and causing microcracks to propagate. Data from a ceramics factory showed that after 50 thermal cycles, the flexural strength of the precast blocks decreased by 35%.
3. Improper Construction and Curing
Uncontrolled water addition directly affects material density. For every 1% increase in water addition during construction, the apparent porosity of the precast blocks increases by 2% and the strength decreases by 10%. At one company, a 3% excess water addition resulted in a 15% cracking rate in the precast blocks after baking.
A poor curing environment accelerates material degradation. When humidity exceeds 80%, calcium hydroxide in the cement hydration products reacts with CO₂ to form calcium carbonate, which expands by 12% and causes surface spalling. Experiments have shown that precast blocks cured at a constant temperature of 20°C are 40% stronger than those cured at 5°C.
NO.02 Systematic Solution: Optimizing the Entire Chain from Raw Materials to Operations and Maintenance
1. Raw Materials: High Purification and Grading Optimization
Using low-alkali raw materials is a fundamental measure. We recommend using premium-grade bauxite (Al₂O₃ ≥ 88%, alkali content ≤ 0.2%) or fused corundum (Al₂O₃ ≥ 99%) calcined in a rotary kiln. After one company switched to a new raw material, the surface pulverization cycle for precast blocks was extended from 3 months to 18 months.
Micropowder filling technology can improve density. Adding 5% α-Al₂O₃ micropowder (particle size < 5μm) can reduce the apparent porosity of precast blocks from 22% to 16% and improve wear resistance by 30%.
2. Manufacturing Process: Precision Control and Additive Innovation
Low-temperature, fast-firing processes can reduce thermal stress. By reducing the sintering temperature from 1450°C to 1380°C and combining it with a 3-hour heat preservation, the thermal shock resistance of precast blocks (water-cooled at 1100°C) increased from 15 to 25 times.
Compound water reducers can reduce water consumption. Using a polycarboxylate-based water reducer instead of calcium lignin sulfonate can reduce the water content from 8% to 6%, while increasing strength by 15 MPa. After implementing this technology at one company, the baking pass rate for precast blocks increased from 85% to 98%.
3. Construction and Maintenance: Standardization and Intelligentization
Construction water quality control is crucial. Using softened water with a pH of 6-8 can reduce cement hydration abnormalities. In one project, excessive water quality (hardness > 300 mg/L) resulted in a 20% efflorescence rate on the surface of precast blocks. Changing the water source eliminated the problem.
The intelligent maintenance system monitors temperature and humidity in real time. By controlling curing room parameters (temperature 20±2°C, humidity 60±5%) through IoT sensors, the 28-day compressive strength of precast blocks increased from 60MPa to 75MPa.
4. Operation and Maintenance Strategy: Preventive Maintenance and Online Monitoring
Pin reinforcement technology enhances spalling resistance. Implanting 8mm stainless steel pins (150mm apart) on the back of precast blocks increases flexural strength by 20% and reduces spalling by 50%.
Infrared thermal imaging can detect potential hazards early. By monitoring the surface temperature distribution of precast blocks, it identifies temperature deviations exceeding 0.5°C and provides early warning of thermal cracking risks. Following implementation at a steel plant, unplanned downtime was reduced by 60%.
NO.03 Industry Practice: Typical Cases and Technical and Economic Analysis
1. Baowu Group’s Blast Furnace Iron Runway Precast Block Renovation
To address the spalling problem of the original precast blocks after just three months of use, a formulation of fused corundum aggregate, silica fume, and low-alkali cement was adopted, combined with an intelligent curing system. After the renovation, the lifespan of precast blocks was extended to 18 months, and the cost of a single replacement was reduced from 500,000 yuan to 200,000 yuan, resulting in an annual maintenance savings of 3 million yuan.
2. Optimization of Shagang Group’s Rotary Kiln Precast Blocks
By adding 0.5% nano-silica (particle size 20nm), the thermal shock resistance of the precast blocks was increased from 10 to 20 times. Furthermore, the use of pin reinforcement technology reduced the shedding rate from 15% to 3%, reducing downtime by 48 hours annually and increasing production benefits by 8 million yuan.
NO.04 Future Trend: Digitalization and Ecological Transformation
With the advancement of Industry 4.0, the field of refractory castable precast blocks is experiencing two major trends:
Digital Twin Technology: By building a full lifecycle model of precast blocks, simulating processes such as thermal stress and chemical corrosion, and optimizing design parameters.
Circular Economy Model: Developing recyclable castable systems, such as by incorporating 30% recycled material from precast waste, achieves performance targets while reducing resource consumption. Surface damage to precast refractory blocks is a result of the combined effects of materials, processes, and the environment, necessitating full-chain optimization to achieve enhanced performance. Companies should consider their specific operating conditions and select targeted solutions to improve equipment efficiency while contributing to carbon neutrality.