Main Characteristics and Features of Electric Arc Furnace Steelmaking
Uses scrap steel or crude steel as the main solid material, eliminating the need for a large ironmaking and coking system;
Wide range of raw material applications, suitable for short-term, intermittent production scheduling;
Utilizes electrical energy for melting (remelting) and heating, easily achieving high temperatures, with convenient and accurate temperature control, beneficial for smelting various steel grades;
Furnace atmosphere (oxidizing, reducing, neutral), vacuum, and pressure are adjustable;
High alloy yield, easy composition adjustment, and narrow control range;
Wide adaptability to various types of steels, high quality, capable of smelting various types of high-quality steel and alloy steel with low P, S, and O content;
Relatively simple equipment, short process flow, small footprint, low infrastructure costs, quick commissioning, and easy pollution control;
High energy consumption, high [N] and [H] content;
Lower productivity than converters, higher consumption of electrodes, refractory materials, etc., compared to other smelting methods.
Electric arc furnaces (EAFs) in steelmaking typically operate in an alkaline, corrosive atmosphere. Therefore, the refractory materials used in EAFs are primarily alkaline refractories, such as MgO-C bricks, pitch-impregnated MgO bricks, MgO-Cr₂O₃ bricks, and MgO-CaO ramming mixes. A smaller portion consists of neutral refractories, such as Al₂O₃-C materials and high-alumina materials.
Overall, the main factors contributing to the damage to EAF refractory materials are: erosion, oxidation, scouring, melting, spalling, and hydration. Among these, oxidation, chemical erosion, and scouring are the most dominant.

01 Chemical Erosion
Acidic components in iron oxide (FeO) or slag, such as SiO₂, react chemically with CaO and MgO as follows:
FeO + MgO = FeO·MgO (1)
SiO₂ + 2MgO = 2MgO·SiO₂ (2)
CaO + SiO₂ + MgO = CaO·MgO·SiO₂ (3)
All of these reactions can turn the furnace lining into molten slag, leading to the destruction of the refractory material.
02 Oxidation
Oxidation is one of the main causes of refractory material erosion in electric furnace linings. During this process, the carbon components in the refractory material are oxidized by oxygen-containing components (such as iron oxide, oxygen, and magnesium oxide), leading to decarburization and damage to the material.
FeO+C(s)=Fe+CO(g) (4)
O2(g)+2C(s)=2CO(g) (5)
MgO(s)+C(s)=Mg(g)+CO(g) (6)
The iron oxide in the slag reacts with the graphite or tar/resin on the hot side of the brick lining, or oxygen erodes the graphite or binder on the cold side of the brick lining. In both cases, the strength of the brick decreases, and it may be eroded by molten slag or steel.
Under the atmosphere of an actual electric furnace, reaction (6) is particularly easy to occur above 1700℃. The generated Mg vapor easily diffuses, causing structural deterioration, which is one of the main factors causing high-temperature damage to magnesia-carbon bricks.
03 Erosion or Mechanical Impact
Physical damage occurs due to the physical wear or erosion of the furnace lining caused by the flow of molten steel or slag over the refractory surface. Erosion is most common at the tapping spout, slag line, electrode port, or exhaust platform of the electric furnace.
Stripping is a complex mechanism of refractory material damage. This is caused by the stress generated in the refractory lining due to rapid heating and cooling. This stress often exceeds the strength of the refractory material, leading to intersecting and penetrating cracks. Fragments of the lining will peel off or completely detach, a common occurrence on the top of electric furnaces.
04 Hydration
Hydration is also a factor contributing to the damage of electric furnace refractory materials. During use, water easily seeps into the furnace cover or walls. Water or steam can corrode the refractory lining. Magnesium oxide (or other basic oxides) reacts with water (or steam) and becomes hydrated as follows:
MgO(s) + H₂O(l/g) = Mg(OH)₂(s) (7)
Reaction (7) leads to a significant weakening of the refractory material’s performance, resulting in poor resistance to slag and molten steel penetration. The above analysis of the causes of damage shows that the refractory materials selected for various parts of the steelmaking electric furnace have the following performance requirements: ① good chemical and volume stability; ② the material composition should not react with molten steel or SiO₂, and should not easily form nodules; ③ it should not be easily wetted or penetrated by molten steel; ④ it should have good resistance to rapid cooling and heating, and should not be easily damaged or spalled off; ⑤ it should have high density, low porosity, and uniform pore distribution, and should not be easily penetrated by molten steel; ⑥ it should have high strength and be able to resist mechanical impact and erosion.
FAQ
What are the core advantages of electric arc furnace (EAF) steelmaking compared to traditional converter steelmaking?
Answer: The main advantages of EAF steelmaking are:
Flexible raw materials: It uses scrap steel as the main raw material, eliminating the need for large ironmaking and coking systems.
Flexible production: Suitable for short-term, intermittent production scheduling.
Precise temperature control: Utilizing electric heating, high temperatures are easily achieved and temperature adjustment is convenient.
Controllable quality: The furnace atmosphere and pressure are adjustable, resulting in high alloy yields, suitable for smelting high-quality alloy steels with low P, S, and O content.
Environmentally friendly and economical: Short process flow, small footprint, low infrastructure costs, and easy pollution control.
Why are basic materials the main refractory materials used in electric arc furnaces?
Answer: Because electric arc furnaces are typically located in an alkaline corrosive atmosphere during operation. To resist chemical corrosion, the furnace lining mainly uses basic refractory materials such as MgO-C bricks (magnesia-carbon bricks), pitch-impregnated MgO bricks, and MgO-CaO ramming mixes, as well as a small amount of alumina-based neutral materials.
What properties should an ideal electric arc furnace refractory material possess?
Answer: Based on the analysis of the damage causes, high-quality electric furnace refractory materials must possess the following six properties:
Good chemical and volumetric stability.
Not easily reacting with molten steel or SiO₂ to form nodules.
Not easily wetted or penetrated by molten steel.
Excellent resistance to rapid heating and cooling (thermal shock resistance).
High density and low porosity.
High strength to resist mechanical impact and erosion.