lmm@magnesiacarbonbricklmm.com

Technical support and construction service team

Classification of binders for refractory castables

Binders refer to substances added to non-plastic granular or fibrous materials to give them workability and green strength or dry strength. In refractory castables, in addition to considering the binding properties of binders, it is also necessary to consider their changes during heating, their reactions with the bound materials at high temperatures, and their effects on the composition, microstructure and properties of the latter. Binders are an important component of castables. Under certain conditions, they are combined in a certain way to harden the castables and gain strength. As the main component that determines the structural strength of castables, binders provide castables with a certain degree of fluidity and demoulding strength, which has a great influence on the performance of castables. There are many binders for castables, and there are many ways to classify them.

refractory castables
refractory castables

Classification by chemical composition and properties

According to chemical properties, they can be divided into two categories: organic binders and inorganic binders.

Inorganic binders can be divided into the following categories according to their chemical composition:

(1) Silicates. Silicate cement, water glass and binding clay.

(2) Aluminates. Calcium aluminate cement (including high purity and low purity), barium aluminate cement, etc.

(3) Phosphates. Phosphoric acid and various phosphates, such as aluminum dihydrogen phosphate, magnesium phosphate, ammonium dihydrogen phosphate, aluminum chromium phosphate, sodium tripolyphosphate, sodium phosphate, etc.

(4) Sulfates. Common ones include aluminum sulfate, magnesium sulfate, etc.

(5) Chlorides. Such as magnesium chloride and brine, polyaluminum chloride, etc.

(6) Sol (or gel) and micropowder. There are silica sol, alumina sol, silica-alumina composite sol,

Organic binders can be divided into:

(1) Natural organic matter or substances separated from natural organic matter. Mainly starch, dextrin, molasses, gum arabic, pulp waste liquid and wood calcium sulfonate, sodium alginate, tar and asphalt, etc.

(2) Synthetic organic matter. Including various resins, such as phenolic resin, epoxy resin, urea-formaldehyde resin, furan resin, etc. In addition, there are polyvinyl alcohol, hydroxymethyl cellulose, ethyl silicate, polyvinyl acetate, etc.

Organic binders can also be divided into two categories: water-soluble and water-insoluble. The residual carbon obtained after carbonization of water-insoluble ones is higher.

Classification by hardening conditions

According to the hardening conditions of castables, they can be divided into three categories:

(1) Hydraulic binder. After adding water and mixing, the castables are cured and solidified through hydration reaction. Various cements are such binders.

(2) Air-hardening binder. It refers to a binder that can solidify and harden under natural drying conditions at room temperature. For example, water glass and phosphates are mostly such binders, and accelerators are usually added. Sometimes drying is also required to obtain higher strength.

(3) Thermosetting binder. It refers to a binder that needs to be baked at a certain temperature (105~350℃) to solidify and harden, such as phenolic resin binder. Sometimes accelerator materials are also needed. For example, when using linear phenolic resin, hexamethylenetetramine needs to be added to harden through the condensation reaction that occurs during heating.

Classification by bonding mechanism

According to the bonding mechanism, it can be divided into six categories: hydration bonding, chemical bonding, coagulation bonding, condensation bonding, adhesion bonding and high-temperature liquid bonding.

Hydration bonding refers to the process of the binder condensing, hardening and gaining strength by hydration reaction at room temperature. Common hydration binders include hydraulic binders such as hydrated alumina and calcium aluminate cement; chemical bonding refers to the process of forming a bond by chemical reaction between the binder and the bonded material or between the binder and the added accelerator to form a physical phase with a bonding effect. Common chemical binders include alkali metal silicates and phosphates; adding a coagulant or adjusting the pH value to the suspension of solid small particles-water system to cause the microparticles to condense and produce a bond is called cohesion bonding. Bonds formed by various colloidal binders and suspension binders belong to this type. Condensation bonding refers to the bonding formed by adding a catalyst or a cross-linking agent to cause the binder to undergo a condensation reaction. Most bonds formed by resin binders belong to this type. Adhesion bonding refers to the bonding formed by connecting solids together through physical or chemical action. It includes the bonding formed by physical adsorption (van der Waals force) and chemical adsorption formed by chemical bonds formed on the surface of solid particles; the second is the bonding formed by the penetration and diffusion of the binder on the surface of the particles to form an interconnected film; and the third is the bonding formed by the double electric layer existing on the interface between the binder and the bonded material, which is bonded together under the action of static electricity. High-temperature liquid bonding is also called ceramic bonding, which is common in dry materials. Boric anhydride or boric acid is most commonly used as a binder for corundum dry materials. Boric anhydride can form a liquid phase with high viscosity at 450~550℃, which can bind corundum particles together. As the temperature rises, alumina can generate 2Al2O3-B2O3 through solid-liquid reaction, and finally generate 9Al2O3-B2O3.

Commonly used binder – calcium aluminate cement

The most widely used binder in current refractory castables is calcium aluminate cement. It is made by mixing aluminous and lime materials in appropriate proportions, then using a melting method or a sintering method, and finally grinding the product into fine powder, that is, alumina cement, also known as calcium aluminate cement, and alumina or alumina and dolomite as raw materials to make aluminate cement containing magnesium aluminum spinel. Since 1916, calcium aluminate cement has been officially used commercially, and it has also begun to be gradually popularized in the refractory industry as a binder for refractory castables.

The main chemical components of calcium aluminate cement are aluminum oxide and calcium oxide, and it also contains a small amount of ferric oxide, silicon dioxide and titanium oxide. Because the raw materials and production processes of calcium aluminate cement are different, the content of various oxides in it is also different. According to its chemical composition, that is, the impurity content, it can be divided into three categories: low purity, medium purity and high purity. Table 1 gives the specific chemical composition classification method.

PropertiesLow purityMedium purityHigh purity
Chemical composition/%SiO₂4.5~9.03.5~6.00.0~0.3
 Al₂O₃39~5055~56 70~90
 Fe₂O₃7~161~30.0~0.4
CaO35~4226~36 9~28

The main phases of calcium aluminate cement are calcium aluminate (CA) and calcium aluminate (CA2). CA has high hydraulic activity. Although the setting rate is not fast, the hardening rate is very fast. It is the main source of the early strength of calcium aluminate cement. The CA content is generally in the range of 40%-70%. If the content is too high, the strength will be mainly concentrated in the early stage. CA2 is more in cement with low CaO content, and the hydration and hardening rate is very slow. The early strength is very low but the later strength is high. CA2 takes a long time to hydrate and harden, and the strength after hydration does not increase with time like CA. If the CA2 content is too high (generally >30%), the cement activity is poor, which will affect the hardening performance of the cement. When the Al2O3/CaO ratio is small, a small amount of C12A7 will be generated in the calcium aluminate cement. Because there are many voids in its structure, the cement hydration and setting speed is very fast, but the strength is not high. C12A7 usually exists in an amount of <2%. Studies have shown that C12A7 can make the hydration rate and hydration degree of CA higher. In addition, calcium aluminate cement also contains a small amount of C2AS, C4AF, and C2S. Table 2 shows the main phases in low-purity, medium-purity, and high-purity calcium aluminate cement and their hydration rates.

Hydration speed Cement purity
Low purityMedium purityHigh purity
Fast hydrationC₁₂A₇C₁₂A₇C₁₂A₇
Medium hydrationCACACA
Slow hydrationCA₂,C₂S,C₄AFCA₂,C₂S,C₄AFCA₂
No hydrationC₂AS,CT,AC₂AS,CT,ACA₆,A

According to the different Al2O3 contents, calcium aluminate cement can also be divided into many types, such as Ca-50, Ca-60, Ca-70 and Ca-80. Ca-50 and Ca-60 cements are also called alumina cements, and their alumina content is generally around 50%, mainly using alumina ore and limestone as raw materials. The alumina content of Ca-70 cement is about 70%, which is pure calcium aluminate cement. It usually uses industrial alumina and calcium oxide as raw materials. It has few impurities, good gelling properties and high refractoriness. Because of its good performance, it is suitable for refractory castables. Ca-80 cement has a higher content of alumina micropowder, which can usually reach more than 80%, so it is also called pure calcium aluminate cement. Compared with Ca-70, it can effectively improve the medium-temperature bonding strength of refractory castables. In summary, the higher the content of alumina in calcium aluminate cement, the better its refractoriness, and it is usually used in refractory materials; the lower the alumina content, the higher the calcium oxide content, the better the hydration performance of the cement, and it is usually used in concrete and chemical building materials industries. In the past few decades, the most widely used calcium aluminate cement in refractory materials is Ca-70.

As a hydration binder, calcium aluminate cement provides sufficient demoulding strength for the castable in a short time after encountering water. It is one of the commonly used binders for castables. Calcium aluminate cement not only affects the strength development of castables through the hydration reaction process and hardening process, but also affects the flow deformation, surface damage, carbonation, post-burning strength, volume, expansion and creep properties of castables. Calcium aluminate cement is widely used in defense, metallurgy, chemical industry, construction and other related industries because of its good strength, high refractoriness and anti-scouring characteristics.

Gel bonding began to be used in the 1980s, mainly using silica sol to replace calcium aluminate cement as a binder for refractory castables. It has most of the shortcomings of low-cement castables and ultra-low-cement castables, and also solves most of their shortcomings. It uses mature sol-gel technology, which has been successfully applied to high-performance ceramics and has some advantages such as easy molding, good uniformity, and low sintering temperature. When silica sol is injected into the castables, the refractory particles will be wrapped by silica gel-gel, and these wrapped particles will form initial strength after drying. After using silica sol binder in corundum castables and aluminosilicate castables, the content of calcium oxide will be reduced, and the high-temperature performance of the castable will be improved. However, its wide application is not as extensive as calcium aluminate cement.

FAQ

What are the technological advantages of using silica sol as a binder in improving the “turnover efficiency” of steelmaking containers?

During the baking process of cement-bonded castables, the removal of physical and chemically bound water is relatively slow, and rapid heating can easily lead to cracking. In contrast, silica sol bonding (a type of cohesive bonding) forms a three-dimensional network gel structure, with a smoother dehydration process and better air permeability. Technically, it can achieve “fast drying” and even “rapid heating,” significantly shortening the baking time of newly constructed containers. Furthermore, because it does not contain CaO, it has better volume stability at high temperatures.

Under the trend of “green steel,” what technological challenges and alternatives do organic binders (such as phenolic resins) face?

Traditional resin binders decompose and produce harmful fumes when heated. Current technological focus is on developing environmentally friendly water-based resins or modified biomass binders. Furthermore, for carbon-bonded refractories (such as mortar for magnesia-carbon bricks), research focuses on how to reduce harmful components in the resin while maintaining its “carbon residue” at high temperatures, ensuring the structural integrity and anti-stripping properties of the material in reducing atmospheres (such as converter and electric furnace environments).

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information