Comparison of Advantages and Disadvantages of Integrated Lining Construction vs. Traditional Lining Design in New Steelmaking Converters

In converter steelmaking, the working conditions of the lining in different parts of the converter vary, resulting in different rates and degrees of corrosion. Based on the different working conditions and causes of corrosion in different parts of the converter lining, the use of refractory bricks of various materials or structures in combination for lining on the same converter is called integrated lining. Integrated lining can avoid shutdowns due to severe localized corrosion, achieving the goal of balanced corrosion and extending the service life of the lining.

The quality of the lining construction is crucial to improving its lifespan. The converter lining consists of an insulation layer, a permanent layer, and a working layer. The insulation layer is generally constructed using asbestos board or refractory fiber; the permanent layer is constructed using tar dolomite bricks or low-grade magnesia-carbon bricks; and the working layer is always constructed using magnesia-carbon bricks. The working layer of the converter is in direct contact with high-temperature molten steel and slag, subjected to chemical erosion by the high-temperature slag, scouring by molten steel, slag, and furnace gases, and mechanical impact during scrap steel addition, making its working environment extremely harsh. During the smelting process, due to varying working conditions in different parts, the corrosion rate of different areas of the working lining also differs. To address this, different types of refractory bricks are used depending on the degree of damage. High-grade magnesia-carbon bricks are used in easily damaged areas, while medium- or low-grade magnesia-carbon bricks can be used in less damaged areas. This results in a more uniform corrosion rate across the entire furnace lining; this is known as integrated furnace lining.With technological advancements, new integrated furnace lining methods offer advantages over traditional methods. They achieve more even corrosion reduction of the furnace lining, extend the overall service life of the converter lining, and improve the converter’s technical and economic indicators.

Problems with Traditional Integrated Masonry Construction:

Arc-shaped Transition Area of the Molten Pool

Traditional masonry construction of the arc-shaped transition area of the molten pool involves tamping the furnace bottom after the outermost layer of magnesia-carbon bricks is laid. Magnesia-carbon tamping material is used to level the triangular area between the lower part of the outermost layer of magnesia-carbon bricks and the surrounding furnace shell using a pneumatic hammer. After the furnace bottom is firmly tamped and leveled using the height of the furnace shell’s spherical crown as a reference, the first layer of leveling bricks is laid. During construction, a level is used to level each brick individually, controlling the horizontal height error to within 2mm. The leveling bricks must be tamped tightly at the front and firmly secured at the back. After laying the first layer of leveling bricks, a pneumatic hammer is used to tamp and level the ramming material in front of the leveling bricks. This leveling material is then used as a reference to build the first layer of magnesia-carbon bricks up to the molten pool. Traditional integrated masonry methods have several drawbacks: complex construction processes, requiring leveling for each layer of leveling bricks, affecting furnace efficiency; stress concentration due to the combined effects of thermal expansion of the furnace bottom bricks and the weight of the leveling bricks themselves; and the presence of brick joints between the leveling bricks and the outermost ring of furnace bottom bricks, which are subject to strong scouring by the molten steel vortex, gradually damaging the brickwork. Combined with thermal stress, this eventually becomes a “weak point.” The ramming material at the bottom of the leveling bricks is prone to loosening and falling off during converter production, and the static pressure of the molten steel can easily lead to “steel leakage” accidents.

Furnace Cap Design

The furnace cap is the area most severely affected by slag erosion, as well as rapid temperature changes and scouring by dust-laden exhaust gases. Therefore, magnesia-carbon bricks with strong slag resistance and thermal shock resistance are used. Traditional furnace cap bricks, composed of magnesia-carbon bricks and magnesia bricks, suffer from several problems: the furnace cap transition lacks a curved shape, leading to severe erosion by flue gas; the magnesia-carbon bricks at the transition position are relatively short, providing limited support to the upper magnesia-carbon bricks; and the gaps between the magnesia bricks and magnesia-carbon bricks, and between the magnesia bricks and the furnace shell, are large, making them prone to loosening.

Bottom-blown brick arrangement design

The radius of the bottom-blown outer ring gas supply bricks in traditional converters is relatively large. For example, in one steel plant, they are distributed on a circumference of 0.76D (D is the diameter of the molten pool) on the working face, too close to the converter’s triangular area. Under normal circumstances, the triangular area is essentially a blind zone for molten steel stirring, where the steel flow is least intense, and the erosion and corrosion of the refractory materials are minimal. However, the trunnion is located above the molten pool, a erosion zone caused by molten steel, and is difficult to slag-accumulate and repair. During blowing, the magnesia-carbon bricks are in a state of slag erosion, making them one of the weakest links in the converter lining. However, with increasing furnace age, an excessively thick or dense slag layer forms above the bottom-blown bricks, hindering the entry of bottom-blown gas into the molten steel. In this state, the bottom-blown gas enters the molten steel through the gap between the working layer and the slag layer at the furnace bottom, entering the triangular zone, which becomes the area of ​​most intense agitation and increases the erosion rate of the furnace lining bricks in this zone. This easily leads to excessively rapid erosion in the triangular zone, increasing the possibility of steel leakage; it alters the bottom-blown gas supply mode, resulting in poor metallurgical performance and increasing the difficulty of furnace bottom maintenance; and severe erosion in the area below the trunnions poses a significant safety risk.

Bottom Brick Thickness Design

The thickness of the converter bottom is crucial for the entire converter service life. It must ensure good bottom blowing permeability while maintaining a reasonable safety thickness. The bottom is subjected to severe erosion from molten steel and slag during blowing, which is the main cause of damage to the magnesia-carbon bricks in this area. Traditional designs use 700-900mm thick magnesia-carbon bricks at the bottom. To ensure bottom safety in the later stages of the service life, bottom blowing permeability bricks are often shut off, resulting in uneven decarburization of the molten steel, higher carbon-oxygen product, and higher production costs.

Optimization of Comprehensive Bridging of New Converter Lining

2.1 Arc Transition Area of the Molten Pool

The converter bottom and molten pool have rapid erosion rates, making them weak points in the converter. The degree of molten pool erosion directly affects the converter’s service life. Using MT-16A magnesia-carbon bricks in the molten pool area, with increased carbon content and the addition of antioxidants, improves the high-temperature strength, slag erosion resistance, and thermal shock resistance of the magnesia-carbon bricks. The connection between the furnace bottom and the furnace body is constructed with an arc, which effectively increases the working thickness of this part. Since there are no joints between the furnace bottom and the molten pool, the penetration and erosion of molten steel are reduced. The transition part is heated evenly without high temperature points. There is no over-oxidation on the surface of the inner arc bricks, and there are no obvious thermal stress concentration points on the outer arc. At the same time, due to the more scientific construction method, the erosion rate in this part will be more uniform. During use, it is beneficial to ensure the integrity of the lining and improve the service life. The arc transition part of the new converter molten pool is shown in Figure 1.

2.2 Furnace Cap Design

After optimization, the furnace cap bricks exhibit the following advantages: 1) The furnace cap bricks are linearly designed, resulting in less resistance to high-temperature flue gas scouring and slag splashing at the furnace cap location, reducing scouring and erosion during the smelting process. 2) The transition area between the furnace body and the furnace cap is uniform, ensuring good gravity transfer of the magnesia-carbon bricks. 3) The magnesia-carbon bricks in the furnace cap are irregularly shaped, reducing gaps between magnesia bricks and magnesia-carbon bricks, and between magnesia bricks and the furnace shell, resulting in a better overall brick shape in the furnace cap area. The specific design of the furnace cap area of the new converter lining is shown in Figure 2.

2.3 Bottom-blown brick layout design

To address the problems of traditional bottom-blown brick layout designs, the layout is optimized. The bottom-blown elements should be positioned away from the impact circle of the top-blown oxygen lance to prevent the top and bottom-blown impact energies from canceling each other out and affecting the mixing effect. The bottom-blown elements should be positioned to facilitate slag splashing and bottom purging processes, maintaining a good mushroom head shape. The bottom-blown gas supply elements should be positioned at the center of the ring bricks to reduce brick cutting and facilitate converter bottom construction. Bottom-blown permeable elements should be avoided below the secondary lance to reduce slag adhesion and measurement interference. Furthermore, considering the impact of charging in the permeable brick area of ​​the bottom, the bottom-blown bricks are arranged on the converter molten pool diameters of 0.48D and 0.32D, respectively. The specific design of the new converter bottom-blown brick layout is shown in Figure 3.

2.4 Bottom Brick Design

Addressing the problems of traditional converter bottom designs, and to improve the bottom’s ability to withstand the severe erosion and wear caused by molten steel and slag during long-term blowing, the magnesia-carbon bricks at the bottom are designed to be approximately 1300mm thick. This ensures both the new converter’s center of gravity meets the requirements of the tilting system and satisfies the requirements for good bottom blowing throughout the converter’s operation.

Conclusions

1) The optimized comprehensive brickwork of the new converter ensures balanced erosion in areas such as the converter cap, arc transition, permeable bricks, and bottom, achieving good control of the converter’s shape. In particular, there are no obvious depressions in the lower part of the trunnion and the molten pool area, creating conditions for safe, stable, and efficient converter production.

2) The optimized comprehensive brickwork of the new converter improves the erosion resistance of various parts of the converter. After 2500 heats of operation, the length loss of the magnesia-carbon bricks in the molten pool is only 0.04mm/heat, reaching a good level.

3) The optimization of the new converter’s integrated masonry design is scientific and reasonable, with advanced and mature technology, and good performance. It reduces the consumption of refractory materials per ton of steel and ensures the effect of combined blowing metallurgy.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information