In steel production, the reheating furnace is an essential piece of equipment in the rolling process. During billet heating, oxidation inevitably occurs, leading to oxidation loss and scale formation on the steel surface.
Oxidation loss not only increases raw material consumption and production costs but also negatively affects steel quality. It can reduce surface quality, influence internal mechanical properties, and lower the overall yield of finished products.
In many rolling mills, the oxidation loss rate during billet heating is around 1.5%, and in some cases even higher. For example, if a steel plant produces 2 million tons of steel per year, a 1.5% oxidation rate means an annual loss of 30,000 tons of steel. Such losses can result in significant economic impact.
Therefore, studying the mechanisms of high-temperature oxidation and implementing effective control measures is extremely important for improving steel quality, reducing production costs, and enhancing the competitiveness of steel manufacturers.
Steel oxidation can occur even at room temperature, but the rate is extremely slow. As temperature increases, oxidation accelerates significantly.
When the temperature exceeds 1150°C, oxidation reactions become much stronger. At 1300°C, the oxidation rate can be several times higher than at 1150°C.
Oxidation loss is closely related to the time the billet remains inside the furnace.
For carbon steel heated at 1100°C, every additional hour in the furnace can increase oxidation loss by 0.3% to 0.5%.
Therefore, excessive residence time in the furnace leads to greater oxidation and material loss.
The atmosphere inside the reheating furnace is one of the most critical factors affecting oxidation.
When the excess air coefficient exceeds 1.2, the concentration of oxidizing gases increases rapidly, which can increase the oxidation rate by more than 40%.
If the oxygen partial pressure is reduced from 4% to 0.1%, the oxidation loss of certain steels can be reduced by more than 70%.
The surface condition of steel billets also plays an important role.
For example, when the surface roughness increases, the contact area between the billet and oxidizing gases increases, accelerating oxidation.
Chemical composition also influences oxidation behavior. Increasing chromium content can improve the compactness of oxide scale and reduce oxidation loss.
Improving Temperature Measurement Accuracy
Accurate temperature measurement during billet charging is important for controlling furnace operation.
High-precision pyrometers can be installed near the furnace charging area to monitor billet temperature in real time. When billets arrive at the entry roller table, the system automatically measures the temperature and transmits the data to the furnace control system.
Rational Control of Heating Temperature
In practical production, the heating temperature can be optimized based on billet size and steel grade.
For example, in low-carbon steel production, the billet temperature can be reduced by about 20°C while still meeting rolling requirements. This helps reduce oxidation while maintaining product quality.
Optimization of Rolling Pass Schedule
Optimizing the rolling pass schedule can improve production efficiency and reduce energy consumption.
In one case study, a steel plant replaced the traditional 3+5 rolling pass schedule with a 3+3 pass schedule. Simulation analysis showed that stress distribution in the billet became more uniform, improving steel quality.
At the same time, the soaking zone temperature of the reheating furnace was reduced by 15°C, which helped decrease oxidation loss.
| 3+3 and 3+5 Pass Mode Comparison Data | ||||
| Pass Mode |
Average TemperatureDrop/℃ |
Exit Temperature/℃ |
Oxidation Burnout Rate/% |
Electrical consumptionof rolling/(kW-h/t) |
| 3+5 passes | 180±15 | 1230±20 | 1.42±0.08 | 38.5±1.2 |
| 3+3 passes | 150±10 | 1200±15 | 1.18±0.06 | 35.2±1.0 |
Burner Parameter Calibration
A dedicated burner calibration system can be used to optimize combustion parameters.
By entering air pressure, gas pressure, temperature, and excess air coefficient into the system, optimal operating conditions can be calculated automatically.
Accurate burner calibration improves fuel efficiency and helps maintain a stable furnace atmosphere.
Improving Valve Control Precision
During furnace maintenance shutdowns, burner valves should be inspected and calibrated.
Technicians measure air and gas pressures at each burner and repair or replace valves that fail to meet operational requirements. This ensures stable combustion and accurate furnace atmosphere control.
Adjusting Burner Nozzle Angle
Adjusting burner nozzle angles can improve gas-air mixing efficiency.
In practical operation, the nozzle angle can be adjusted to approximately 80°–85°, and airflow intersection angles can be controlled within 10°–20°. This improves combustion efficiency and reduces oxidation risk.
Removal of Rust and Surface Impurities
Mechanical grinding combined with chemical cleaning can effectively remove rust and contaminants from billet surfaces.
After grinding, billets can be immersed in cleaning solutions containing rust-removal agents and degreasers. High-pressure water cleaning is then used to remove remaining impurities.
This process significantly reduces oxidation during heating.
Improving Surface Smoothness
Polishing billets with specialized polishing wheels helps reduce surface roughness.
A smoother billet surface decreases the contact area with oxidizing gases and reduces oxidation reactions during heating.
At the same time, smoother surfaces improve downstream processing quality.
Optimization of Billet Charging Gap
Optimizing billet charging gaps can improve heating uniformity.
By analyzing historical production data and furnace operating parameters, an intelligent model can determine the optimal billet spacing. For example, billets with a width of 1200 mm may require an optimal charging gap of approximately 400 mm.
Increasing Production Rhythm
Upgrading motors and optimizing roller table control systems can increase billet transport speed.
Shorter furnace residence time reduces oxidation loss and improves production efficiency.
| Pre- and post-improving steel loading and steel rolling velocity Unit:m/s | ||
| Improvement Item | Before Improvement | Improved |
| Steel Roll Conveyor Speed | 0.8 | 1.2 |
| Steel Outlet Roller Speed | 1.8 | 2 |
Optimizing Billet Discharge Timing
By upgrading furnace control systems and improving communication between furnaces and rolling mills, billet discharge timing can be optimized.

Conclusion
This reduces billet waiting time inside the furnace and improves overall production continuity.
High-temperature oxidation loss in reheating furnaces is influenced by several factors, including heating temperature, furnace atmosphere, residence time, and billet surface condition.
By optimizing heating parameters, improving furnace atmosphere control, enhancing billet surface treatment, and upgrading furnace operation systems, steel plants can effectively reduce oxidation loss.
These measures not only improve steel product quality but also reduce production costs and enhance production efficiency.
An oxidizing furnace atmosphere with high oxygen content increases the oxidation rate of steel billets.
Optimization of heating temperature, furnace atmosphere, billet surface treatment, and furnace operation can effectively reduce oxidation loss.
Proper billet spacing improves heat distribution and reduces uneven heating and oxidation.