During the service process, the ladle lining refractory materials of the refined ladle are in direct contact with high-temperature molten steel and slag. At the same time, they are also faced with drastic changes in temperature and atmosphere, as well as smelting operations such as alloying and stirring. The service environment is complex and harsh, so they often suffer serious damage. Generally speaking, the use environment of the working layer refractory materials can be summarized as follows: the refining temperature is high (over 1600℃), and the molten steel stays in the ladle for a long time; for different refining processes outside the furnace, there are argon blowing, oxygen blowing stirring and vacuum environments; the alloy components added to the smelting of various alloy steels cause the slag composition to change greatly during the refining process, and it is difficult to suppress the erosion of the slag by matching the slag and refractory components; the various operations of the refining process are mostly intermittent, and the thermal stress cycle further leads to thermal spalling damage of the working layer material.
According to the causes of damage, the damage of the ladle refractory materials can be divided into the following aspects:
1) Chemical action
-erosion of molten steel and slag components on refractory materials
——Damage caused by the reaction of the refractory material itself under high temperature, such as the volume effect caused by the phase change caused by the formation of new minerals and the volatilization under vacuum.
2) Physical effect
——The scouring and dissolution of refractory materials by high temperature molten steel.
——The thermal shock caused by the repeated action of molten steel on refractory materials causes the cracking and spalling of refractory materials in the working layer.
——Damage caused by the thermal expansion effect of refractory materials themselves.
3) Damage caused by improper human operation
Due to the different environments faced by refractory materials in different parts of the refining ladle, the types of damage are also different. In the ladle, the refractory materials in the slag line are mainly damaged by the melting of slag, while the scouring damage and thermal spalling damage of the ladle wall and ladle bottom are more common. If a castable with a larger critical particle size is used on the ladle wall, it is easier to cause structural spalling due to the scouring effect of molten steel and thermal stress cycle. Figure 1 below shows the main forms of damage in different parts of the ladle.