lmm@magnesiacarbonbricklmm.com

Technical support and construction service team

Damage mechanism of zirconia sizing nozzle in use

The damage process of zirconia sizing nozzle is the complex physical and chemical interaction between it and steel slag and molten steel at high temperature. The damage mechanism of zirconia sizing nozzle is discussed from the perspective of high-temperature physical and chemical reactions.

Physical damage

① Thermal shock damage.

In the actual steel pouring process, the zirconia sizing nozzle is subjected to severe thermal shock due to the high pouring temperature and rapid heating, and the internal heating of the nozzle is uneven. Thermal shock causes large thermal stress inside the sizing nozzle. As the steel pouring process proceeds, this non-uniform thermal stress causes potential defects or damage to the internal structure of the nozzle, and even produces micro cracks. The structural damage caused by thermal shock reduces the strength and erosion resistance of the nozzle, and also provides a way for molten steel and slag to penetrate and erode the inside of the nozzle. Particularly severe thermal shock can directly cause macro cracks in the sizing nozzle, or even burst directly at the moment of pouring. Therefore, the thermal shock of molten steel is the most serious damage to the sizing nozzle during the nozzle damage process.

② Mechanical scouring damage.

The mechanical scouring of molten steel on the nozzle is very serious. Although molten steel is a high-viscosity liquid, it has a serious thermal scouring on the nozzles due to its high specific gravity, high temperature and fast flow rate. The high temperature produces a large temperature gradient in the cross section of the nozzles wall, which greatly reduces the strength of the nozzles wall in contact with the molten steel. According to estimates, the speed of molten steel passing through the nozzle is 3-5m/s, and it often carries a rotating vortex. These factors have aggravated the erosion of the nozzles by molten steel.

Chemical damage

① Zirconia dissolution.

The main chemical components of the zirconia sizing nozzle are ZrO2, a small amount of stabilizers (CaO, MgO, Y2O3, etc.) and trace impurities. Pure zirconia undergoes a transformation from monoclinic phase to tetragonal phase at 900~1200℃, namely, martensitic phase transformation. This phase transformation easily causes volume change, and thus pure zirconia products cannot be produced. Most of the sizing nozzles currently used use CaO and MgO as stabilizers. During the use of stabilized zirconia, molten steel and inclusions in the molten steel (such as MnO2, SiO2, MgO, Al2O3, etc.) are prone to react with stabilizers (CaO, MgO) to form multi-element low-melting-point oxide melts that flow away with the molten steel. Zirconia destabilizes and decomposes due to the dissolution of the stabilizer, and becomes small monoclinic phase particles that flow away with the molten steel.

② Penetration and erosion of molten steel and slag.

Molten steel corrodes the zirconia sizing nozzle to generate low-melting-point oxides, and the liquid phase generated by the reaction gradually penetrates into the nozzles through the pores. The higher the porosity, the more liquid phase penetrates, and the zirconia becomes unstable due to the desolvation of the stabilizer, which intensifies the decomposition process, and smaller round monoclinic zirconia particles enter the melt. The desolvation of the stabilizer and the penetration of the multi-phase liquid phase destroy the ceramic bonding of the zirconia on the nozzle surface, reducing the bonding strength between them. When the bonding strength is not enough to resist the erosion of molten steel, it is easy to be washed away by the molten steel, causing the nozzle to expand during use.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time