lmm@magnesiacarbonbricklmm.com

Technical support and construction service team

Definition of refractory castables bonding system and bonding methods

Refractory castables bonding agent

The sum of the bonding agent in the refractory castables and other substances such as dispersants and retarders that can assist the bonding agent and make it fully play its bonding role is called the bonding system of the refractory castable material. Due to its weaker strength compared to the aggregate, the strength of the hardened body of the bonding agent in the refractory castable can determine the strength of the refractory castable product. In addition to the physical and chemical properties and particle grading of the aggregate and powder used in the refractory castable material, the bonding system of the refractory castable is also a crucial factor that can affect the construction and use performance of the refractory castable.

As an important component of the bonding system, the selection of the bonding agent should try to meet the following two conditions: 1. It can provide a certain bonding strength for the refractory castable product during the construction and maintenance process; 2. It can make the matrix produce an enhanced reaction during the use process after the construction is completed.

1. Hydration bonding – refractory castables

Using cement and other hydraulic binders to meet the requirements of specific temperature and humidity to produce hydration reactions, and generate hydration products that can produce gelling effects to bond refractory castables. This bonding method is called hydration bonding. Typical hydraulic binders include calcium silicate cement, calcium aluminate cement, hydraulic alumina, etc. Among them, calcium aluminate cement is the most widely used.

The composition of calcium aluminate cement is shown in Table 1. The chemical composition is mainly Al2O3 and CaO. Its mineral composition is monocalcium aluminate CaO·Al2O3 (CA), calcium dialuminate CaO·2Al2O3 (CA2), calcium heptadecaluminate 12CaO·7Al2O3 (C12A7), calcium feldspar 2CaO·Al2O3·SiO2 (C2AS), tetracalcium aluminoferrite 4CaO·Al2O3·Fe2O3 (C4AF), etc. Light yellow high alumina cement with low iron content and white high alumina cement with low calcium content are often used as binders in the refractory field.

Cement types Chemical composition (%)Al₂O₃/CaOMain mineralsAppearance color
SiO₂Al₂O₃ Fe₂O₃  CaO
High alumina cement 13~935~45  10~17  36~400.85~1.3CA、C4AF、C₂ASGray to black
High alumina cement 2  3~650~65  1~329~40  1.2~2.2CA、C₂ASLight yellow
Low calcium high alumina cement0~1.460~80  0~117~27   2.8~4.7CA、CA₂,α-Al₂O₃White

As a hydration binder, hydraulic alumina has also been widely used. Hydraulic alumina is an alumina intermediate product generated when aluminum hydroxide is rapidly dehydrated. It contains a certain amount of structural water and is a mixture of boehmite and various alumina variants such as ρ-Al2O3. One advantage of using hydraulic alumina as a hydration binder for high-alumina refractory castables compared to calcium aluminate cement is that it is conducive to the purification of refractory castables.

2. Chemical bonding

The binder and the raw material or the accelerator added to the refractory castable can react chemically under certain temperature conditions to generate a reaction product that can produce polymerization to bind the refractory castable. This bonding method is called chemical bonding. Phosphoric acid is often used as a chemical binder because it can ionize phosphate, monohydrogen phosphate and dihydrogen phosphate ions, and combine with the refractory castable matrix or the added accelerator to form a compound phosphate with cementing ability. In addition, sodium silicate (water glass) is also often used as a chemical binder.

3. Coagulation bonding

The ultrafine powder or flocculent particles introduced into the refractory castable have a particle size of submicron scale. When they are in contact with each other or approach each other in the refractory castable and the distance is reduced to nanometer scale, they coagulate due to the existence of intermolecular forces or hydrogen bond bridging, resulting in bonding. This bonding method is called coagulation bonding.

Since coagulation bonding mainly relies on the addition of clay micropowder, silicon micropowder, alumina micropowder, etc., the amount of impurities introduced by the binder in the refractory castable is less than that of other bonding methods, which is beneficial to improving the high-temperature performance of the refractory castable. Due to its small size, the fine powder can play a gap-filling role in the refractory castable, improve the density of the refractory castable, and reduce the amount of water required for the refractory castable. This makes it so that the hydration products containing structural water will not be generated in large quantities in the coagulated refractory castable, and the volatilization and decomposition components are less, which is beneficial to the maintenance of the structure and strength of the refractory castable after heating. In addition, the fine powder has a relatively high surface activity, which can reduce the temperature required for sintering and achieve energy saving.

FAQ

Why have “low-cement (LCC)” or “ultra-low-cement” bonding systems become the mainstream choice for steel mills?

A: Traditional high-cement castables contain a large amount of calcium oxide (CaO), which easily reacts with aluminum and silicon components at high temperatures to form low-melting-point substances, reducing refractoriness. Low-cement bonding systems, through the introduction of micronization technology, significantly reduce cement usage. For steel mills, this not only significantly improves the castable’s resistance to slag erosion and high-temperature strength, but also, due to its low porosity, effectively prevents molten steel penetration, making it a core material for ladle and tundish linings.

How much time can castables bonded with “silica sol” save during steel mill maintenance?

A: Traditional cement-bonded (hydration-bonded) materials experience slow moisture removal during baking, and rapid heating can easily lead to cracking. Silica sol bonding, on the other hand, is a cohesive bonding system; its resulting network structure has excellent permeability and does not contain water of crystallization. This means steel mills can use faster heating curves for baking, even achieving “rapid baking,” significantly shortening the time from equipment maintenance to production and improving production efficiency.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time