lmm@magnesiacarbonbricklmm.com

Technical support and construction service team

Main Factors Affecting EAF Magnesia Carbon Brick Life

In modern electric arc furnace steelmaking, the service life of the furnace lining is directly related to production efficiency, energy consumption, and refractory cost control. Among all refractory products, EAF magnesia carbon bricks play a critical role because they must withstand extreme temperatures, slag corrosion, thermal shock, and arc radiation during continuous steelmaking operations.

The primary refractory materials used include: bottom electrode sleeve bricks, small furnace bottom ramming mix, furnace bottom ramming mix, magnesia carbon bricks for electric arc furnaces, EAF gunning mix, furnace roof castables, taphole gunning mix, and taphole filler, etc.

EAF magnesia carbon bricks inside a UHP DC electric arc furnace

Baosteel’s 150-ton UHP DC electric arc furnace was imported from CLECIM, France, and utilizes water-cooled steel bar bottom electrodes. It has a power rating of 99 MVA and integrates a series of advanced technologies, including oxygen lance melting assistance, a “one-power-source-two-furnaces” configuration, water-cooled furnace walls and roofs, bottom argon stirring, foamy slag submerged arc operation, and Eccentric Bottom Tapping (EBT).

The main refractory materials currently used in Baosteel’s 150-ton EAF are as follows:

ItemMaterialPerformance Requirements
Bottom Electrode Sleeve BrickMagnesia-AluminaExcellent thermal shock stability and superior high-temperature corrosion resistance.
Furnace Bottom Ramming MixMagnesia-CalciaGood sintering performance,slag resistance,and low high-temperature linear  shrinkage.
Furnace Lining Magnesia- Carbon BrickMagnesia-CarbonSuperior thermal spalling and high-temperature slag resistance,good oxidation resistance.
Gunning MixMagnesiaGood adhesion and slag resistance,higher high-temperature bonding strength.
Taphole BrickMagnesia-CarbonSuperior steel erosion resistance,good thermal spalling and oxidation resistance,good slag resistance.
Small Furnace RoofCorundumSuperior thermal spalling resistance,good slag resistance and water hydration resistance.

Main Factors Affecting the Service Life of Ultra-High Power (UHP) DC Electric Arc Furnaces and Magnesia Carbon Bricks

Influence of High-Temperature Thermal Effects on Magnesia Carbon Brick Performance

The smelting temperature is generally above 1600°C, which significantly impacts the furnace service life. Furthermore, due to the “one-power-source-two-furnaces” design, the furnace lining must withstand rapid cooling and heating cycles (thermal shock). While this phenomenon is unavoidable during the smelting process, efforts should be made to minimize the intensity and duration of high-temperature thermal exposure.

For high-performance magnesia carbon bricks, repeated thermal cycling can cause oxidation of graphite and structural stress inside the refractory matrix. Therefore, selecting high-density MgO-C bricks with excellent thermal shock resistance is essential for extending EAF lining life.

Practical measures include rapid furnace patching and charging, ensuring normal equipment operation, and minimizing thermal downtime.

Influence of Chemical Erosion on EAF Refractory Bricks

Various chemical reactions occur throughout the steelmaking process, particularly at the slag-steel interface. The furnace lining refractories are highly susceptible to spalling under the influence of these chemical reactions.

Chemical erosion is closely related to the composition and fluidity of the slag. When the content of acidic or semi-acidic oxides—such as SiO2, P2O5, Al2O3, or Fe2O3—is high in the slag, MgO reacts readily to form corresponding magnesium silicates or magnesium aluminates.

The impact of slag fluidity on chemical erosion is primarily manifested in two ways: thin slag with low alkalinity leads to violent chemical reactions and causes bath turbulence, which easily increases the thermal load on the lining; conversely, thick slag makes it difficult to heat the bath, necessitating extended high-temperature smelting times, which also accelerates lining damage.

Furthermore, chemical erosion is also related to the elemental composition of the molten steel. When smelting steels with high concentrations of Mn, Si, W, or very low carbon content, or when the steel contains trace amounts of elements like Pb and Zn, the erosion of the furnace lining is further exacerbated.

For example, when the temperature exceeds 1600°C and the manganese content in the steel is above 10%, Mn will react with the SiO2 in the refractory material as follows:

SiO2(s)+2[Mn]=[Si]+2(MnO)

SiO2(s)+(MnO)=(MnO·SiO2)

While these reactions occur, the softening point of the refractory material will drop to 1150–1250°C. Therefore, when smelting steel grades such as ZGMn (high-manganese steel), the smelting temperature must not be too high, and the operation must be rapid and precise.

When smelting high-silicon steel, the slag contains a correspondingly high level of SiO2, which reduces the slag basicity (alkalinity) and erodes the furnace lining. Consequently, tapping should be performed as quickly as possible after adding large amounts of ferrosilicon to the furnace.

In the case of high-tungsten steel, tungstate ions appear in the molten steel, which also have a corrosive effect on the furnace bottom. Under the same conditions, when smelting very low-carbon steel, the high content of [FeO] reacts with the SiO2 in the refractories to form low-melting-point compounds, which inevitably causes severe erosion of the lining.

Lead (Pb) severely erodes the furnace bottom and can even lead to catastrophic furnace breakout accidents. Zinc (Zn) is also highly detrimental; its oxides specifically tend to accumulate in the pores of the refractory material, leading to expansion and subsequent cracking.

For this reason, many steel plants now prefer high-purity magnesia carbon bricks with improved slag resistance and low porosity to reduce chemical attack and extend refractory campaign life.

Influence of Arc Radiation or Reflection on EAF Magnesia Carbon Bricks

Electric arc furnace steelmaking relies on converting electrical energy into thermal energy to melt cold scrap and heat the molten bath; this energy conversion and transfer are achieved via the electric arc. The radiant or reflected heat from the arc also acts upon the furnace lining, causing the refractory materials to soften.

Currently, although the impact of arc radiation or reflection on lining life cannot be entirely avoided during the smelting process, it can be minimized through various methods. For instance, during charging, solid cold scrap should be distributed rationally within the furnace so that the arc can be “shrouded” by the steel charge shortly after power-on.

During the smelting process, forming a foamy slag as early as possible to submerge the arc can also significantly reduce the damage to the furnace lining caused by arc radiation or reflection.

For modern EAF operations, using anti-oxidation magnesia carbon bricks in high-radiation zones can effectively improve refractory durability and reduce unexpected shutdowns.

Influence of Mechanical Collision and Vibration on Furnace Lining Refractories

Irrational charging and material distribution—such as failing to place light scrap underneath heavy materials or lifting the charging basket too high—can cause the furnace bottom and banks to suffer from collisions, vibrations, and impacts from large, heavy pieces of scrap, leading to pits and hollows.

If the charging process is unguided or the crane operation is abnormal, the charging basket may tilt or drag, causing physical damage to the furnace walls. Furthermore, loose selection of steel scrap may lead to severe explosions during the melting period, all of which shorten the service life of the furnace lining.

Additionally, the high noise levels in the smelting shop and the resulting impact of noise waves are another factor contributing to lining damage.

To reduce mechanical wear, many steel producers adopt wear-resistant magnesia carbon bricks with higher compressive strength and optimized carbon content for critical impact areas.

Influence of Operational Proficiency on EAF Refractory Service Life

During the smelting process, low-level operational skills pose a significant threat to the furnace lining. Improper oxygen blowing can be hazardous, as the temperature at the oxygen lance tip reaches as high as 2100°C; if the oxygen flame is reflected off large pieces of scrap toward the water-cooled furnace walls, it can easily cause leakage.

Incorrect power regimes may lead to excessively high temperatures in the early stages or post-reduction temperature spikes, causing severe damage to the refractory materials. Improper implementation of slag-making regimes—such as having an oxidizing slag that is too thick and viscous combined with low-temperature ore addition—causes CO bubbles to be trapped initially and then erupt violently.

If the slag becomes too thin during the reduction period for any reason, it leads to severe arc reflection, which also accelerates the destruction of the lining.

Poor control of chemical composition can lead to over-oxidation and subsequent overheating of the molten steel, which not only extends the smelting time but also reduces the service life of the furnace lining.

Therefore, in addition to selecting premium EAF magnesia carbon bricks, stable operating procedures and experienced furnace control are equally important for achieving longer refractory campaign life.

Conclusion

The service life of Ultra-High Power (UHP) DC electric arc furnaces is influenced by multiple interacting factors, including high-temperature thermal shock, chemical erosion, arc radiation, mechanical impact, and operational practices. Among all refractory materials used in EAF steelmaking, magnesia carbon bricks remain one of the most critical components because they directly determine furnace stability, safety, and production efficiency.

To improve furnace lining performance and reduce refractory consumption, steel plants should optimize slag control, shorten unnecessary high-temperature holding time, improve charging practices, and select high-quality MgO-C bricks with excellent thermal shock resistance, slag resistance, and oxidation resistance.

With the continuous development of modern electric arc furnace steelmaking technology, advanced EAF magnesia carbon brick solutions will continue to play a vital role in extending furnace campaign life, reducing downtime, and lowering steel production costs.

FAQ

What are magnesia carbon bricks used for in electric arc furnaces?

Magnesia carbon bricks are mainly used in EAF sidewalls, slag lines, and hot spots because they provide excellent thermal shock resistance and slag corrosion resistance.

Why do EAF magnesia carbon bricks wear out quickly?

Rapid wear is usually caused by thermal shock, chemical slag attack, arc radiation, oxidation, mechanical impact from scrap charging, and improper furnace operation.

How can the service life of MgO-C bricks be extended?

The service life can be improved through proper slag control, optimized furnace operation, faster tapping, foamy slag practice, and selecting high-quality refractory materials.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information