The tundish is a device for molten steel transition between the ladle and the crystallizer. The main tasks of the tundish are: (1) diverting molten steel: for multi-stream continuous casting machines, the molten steel is distributed to each crystallizer through the tundish; (2) stabilizing the flow: reducing the static pressure of the molten steel, maintaining a stable liquid level in the tundish, and smoothly injecting the molten steel into the crystallizer; (3) storing molten steel: when replacing the ladles during multi-furnace continuous casting, the casting speed is not reduced to create conditions for multi-furnace continuous casting; (4) purifying molten steel: during a long casting time, the temperature of the molten steel is kept basically unchanged, which promotes the further floating of inclusions in the molten steel, prevents the molten steel from contacting with the air, and avoids oxygen and nitrogen absorption.tundish refractory lining
Composition of refractory materials for tundish lining
The composition of refractory materials for lining of tundish generally includes the following parts:
(1) Insulation layer (10-30 mm), which is adjacent to the steel shell of the tundish and is usually made of ceramic fiberboard, insulation bricks or lightweight castables. The best effect is ceramic fiberboard, which has low thermal conductivity and is easy to lay.
(2) Permanent layer (100-200mm), which is in contact with the insulation layer and is generally made of clay bricks. The integral permanent lining is the most common, and the castable is generally a high-aluminum or mullite self-flowing castable.
(3) Working layer (20-50mm), which is in contact with molten steel and is a key part. Insulation boards or coatings are now commonly used. Insulation boards are generally made of siliceous, magnesium, and forsterite; coatings are made of magnesium, magnesium chromium, and magnesium calcium. The coating is sprayed mechanically or applied manually.
(4) Seat bricks, which are embedded in the bottom of the tundish and used to install the tundish water outlet, are usually made of high-aluminum.
(5) The bottom of the ladle is made of the same material as the working layer. The working layer of the bottom of the tundish is easily damaged by the impact of molten steel and requires corrosion resistance and wear resistance. Generally, high-aluminum bricks or dense high-aluminum bricks and aluminum-chrome bricks are used, and special large-scale high-strength tar-magnesia bricks are also used. Zircon bricks or prefabricated blocks are used to strengthen the impact area of molten steel.
(6) The cover covers the tundish and can play a role in heat preservation and molten steel splashing. The material used is clay or high-aluminum castables as the cover.
(7) Slag retaining wall (weir), which is built in the tundish and can be a single wall or a double wall. The material of the slag retaining wall weir is usually high-aluminum bricks, which can also be made into prefabricated blocks. Its purpose is to retain. In order to improve the cleanliness of molten steel, a molten steel filter can also be set on the slag retaining wall.
Function of the tundish
The continuous casting tundish was originally used for molten steel insulation, and its main purpose was to distribute and rectify the molten steel. With the successful development of molten steel slow cooling, molten steel reheating technology, argon sealing technology, gas stirring technology, and removal of non-metallic inclusions in molten steel, the continuous casting tundish has become the most important refining container in the final stage of the steel smelting process, and is developing towards large-scale.
1. Purification function
In order to produce high-purity clean steel, porous air-permeable bricks are installed at the bottom of the tundish, or porous tubular gas distributors are embedded between the working layer and the permanent layer, or porous bricks are installed on the slag retaining wall for argon blowing, so that argon bubbles float evenly from the bottom, promoting the removal of inclusions. These devices can eliminate the hydrogenation of molten steel in the early stage of pouring, reduce oxide inclusions in molten steel, and reduce defects caused by Al2O3 inclusions on tinplates.
2. Temperature adjustment function
In order to make the temperature difference of molten steel in the front, middle and late stages of the tundish less than 5℃ during the pouring process, close to the liquidus temperature, expand the equiaxed crystal zone of the ingot, and reduce the center segregation, measures such as adding small pieces of scrap steel to the tundish and spraying iron powder can be taken to adjust the temperature of the molten steel.
3. Composition fine-tuning
The center hole of the tundish plug rod feeds aluminum, titanium, boron and other core wires into the crystallizer to achieve fine-tuning of the micro-alloy composition in the steel, which not only improves the recovery rate of easily oxidized elements, but also avoids nozzle blockage.
4. Refining function
Add double-layer slag to the surface of the molten steel in the tundish to absorb the floating inclusions in the molten steel, or feed calcium wire in the tundish to change the Al2O3 inclusion morphology to prevent nozzle blockage.
5. Heating function
Using induction heating and plasma heating in the tundish, the pouring temperature of molten steel can be accurately controlled at ±3~5℃. The tundish is heated at the beginning of continuous casting and at the end of ladle casting to compensate for the decrease in molten steel temperature and keep the molten steel temperature near the target. This is conducive to the stability of casting operation and improves the quality of the ingot. At the same time, during the normal casting period, appropriate heating can compensate for the natural cooling of the molten steel. The heating methods are induction heating and plasma heating.
Tundish is developing towards large-scale
Currently, the capacity of the tundish of slab continuous casting machine is gradually developing towards large-scale. The advantages of increasing the capacity of the tundish are as follows: (1) Prolonging the residence time of molten steel in the ladle is conducive to the floating of inclusions; (2) When changing the ladle, the pulling speed is not reduced to maintain the stability of the tundish casting, and the vortex is prevented from being generated when the liquid level is lower than the critical value, and the slag is drawn into the crystallizer; (3) The molten steel level is stable during the entire casting process, which is conducive to smooth operation; (4) The capacity of the tundish is increased, which is conducive to reducing metal loss and reducing operating costs.
The new tundish adopts a double-shell ladle and ladle cover with vacuum insulation, supplemented by anti-oxidation coating insulation technology and permanent layer castable with low thermal conductivity. The original intention of its development is to use the vacuum insulation principle to reduce the heat dissipation of the tundish during the pouring process, increase the insulation effect of the tundish, and then reduce the tapping temperature, save energy and material consumption in the steelmaking process, and achieve the goal of low superheat constant temperature pouring, thereby achieving the purpose of environmental protection, energy saving, and stable production. Due to the low thermal conductivity of the vacuum cladding, the anti-oxidation coating and the insulation type castable further reduce the thermal conductivity of the cladding refractory material, thereby achieving significant effects such as reducing the temperature drop during the continuous casting process and reducing the temperature of the tundish shell and cladding cover.refractory materials
FAQ
How can the overall cost of a steel mill be reduced by optimizing the configuration of the tundish permanent layer?
Damage to the permanent layer results in extremely high repair and replacement costs and impacts production cycles. The current optimization direction for steel mills is as follows:
Selecting high-alumina spinel castables: This material has better thermal shock resistance and spalling resistance, and can withstand thousands of thermal cycles.
Strengthening the insulation layer design: Adding nano-level insulation boards or ceramic fiber boards between the permanent layer and the cladding shell reduces heat loss. This not only reduces energy consumption per ton of steel but also effectively lowers the temperature of the tundish shell, preventing deformation of the cladding shell due to thermal fatigue, thereby extending the service life of the hardware.
When pursuing “long-life continuous casting,” what is the most common failure risk of the tundish working layer?
Answer: The most critical risks are slag line erosion and structural collapse.
Due to extended continuous casting times (e.g., exceeding 20-40 hours), the chemical erosion of the slag line in the working layer (dry refractory) by the molten slag intensifies. If the material’s slag resistance is insufficient, it can lead to lining perforation or even burnout of the permanent layer. Steel mills typically address this by increasing the purity of magnesium oxide (MgO) in the dry refractory or by locally using reinforced refractory materials at the slag line location to ensure the integrity of the lining throughout the continuous casting cycle.