How should the vulnerable parts of the arc furnace lining be properly repaired?

Damage to the lining

During the smelting process, the furnace body is in a high temperature state, and the lining is constantly subjected to chemical erosion and mechanical scouring at high temperature. After each furnace of steelmaking, the lining is damaged to varying degrees. Therefore, the furnace must be repaired in time after each furnace is tapped. This is an important measure to ensure the normal smelting and extend the furnace life.

The lining includes the furnace wall, furnace bottom and furnace top. Among them, the furnace wall has the lowest lifespan and has the worst working conditions. It is not only close to the arc and has a high temperature, but is also susceptible to severe erosion by the slag.

The lining is generally composed of alkaline materials. The alkaline oxides in the slag (such as CaO, MgO, MnO) have little erosion effect on the furnace lining, while the acidic oxides in the slag (such as SiO2, TiO2, ZrO2, P2O5, etc.) have a large erosion effect on the lining. The furnace age is directly related to the w (SiO2) in the slag. The basicity of the basic arc furnace slag is generally between 2 and 4, which makes the slag have a smaller erosion ability and a higher impurity removal ability.

The furnace lining is seriously damaged or the magnesia sand used for repairing the furnace is not completely sintered and enters the slag, resulting in a large increase in MgO particles in the slag.

The fluidity of the slag becomes poor, which directly affects the chemical reaction between slag and steel, increases the inclusions in the steel, and seriously reduces the steel quality.

A steel company's 2500m³ blast furnace lining wet injection project

The main purpose of repairing the furnace is to repair the vulnerable parts in the furnace, which mainly includes:

01 Furnace wall slag line part

This part of the furnace lining close to the slag layer in the steelmaking furnace is called the slag line part of the furnace lining because it is often in contact with the steelmaking slag. The slag contains calcium oxide (CaO), silicon dioxide (SiO2), ferrous oxide (FeO), calcium fluoride (CaF2), manganese oxide (MnO), aluminum oxide (Al2O3), etc. At high temperatures, the acidic oxides in the slag react chemically with the alkaline furnace lining to form low-melting point compounds, which reduce the refractoriness of the furnace lining. In addition, the physical scouring effect of the slag flow, so the slag line part of the furnace lining is severely damaged, and the slag line near the electrode is more seriously damaged due to the high-temperature radiation of the arc light.

02 Furnace wall hot spot area

The arc temperature is about 4000℃, and the area of ​​the furnace wall closest to the electrode is a relatively high temperature area, often called the hot spot area. The arc light radiates on the furnace wall and withstands a temperature of more than 1700℃. The alkaline furnace lining is built with magnesia bricks or magnesia sand knotted, its refractoriness is about 2000℃, but the softening deformation temperature is only about 1500℃, so the furnace wall in the high temperature area near the electrode is easily damaged.

03 Furnace door and steel outlet

The furnace door is frequently opened and closed, and the drastic temperature changes damage the refractory material at the furnace door. The steel outlet is damaged by the erosion and scouring of high-temperature molten steel and slag.

From the perspective of furnace repair materials, there are dry repair and wet repair materials. The furnace repair materials are magnesia sand [w (MgO)>78%] or roasted dolomite, and tar (hydrocarbon) is used as a binder for dry repair. The binder for wet repair is brine (MgCl2·xH2O) or water glass (Na2SiO4·yH2O), which is often used in places where the furnace lining is severely damaged or has a large slope and is difficult to repair. The ratio of asphalt and magnesia sand is about 1:10, and the amount of brine, water glass or magnesia sand should be kneaded into a ball without looseness.

Throw the furnace repair material to the eroded area, and the heat energy of the furnace lining will sinter the furnace repair material and the furnace lining into a whole. When the furnace is repaired with a mixture of magnesia and asphalt, the liquid asphalt is filled between the magnesia at high temperature, decomposed and volatilized, and the remaining is fixed carbon, which is used as a skeleton to lock the magnesia particles into a whole. Carbon only volatilizes above 4000℃. When wet repair is used, the water of MgCl2·xH2O or Na2SiO4·yH2O evaporates at high temperature, and MgO·MgCl2 compounds are formed in the gaps between the magnesia, which plays a role in locking the magnesia.

The principle of repairing the furnace is high temperature, thin repair, and fast repair. Minimize high temperature radiation heat dissipation as much as possible, and operate quickly.

After the steel is discharged, immediately use a shovel to fill the two sides of the steel outlet and the furnace slope with the repair material, so that the heat loss is less, and then use a large shovel to fill the two sides of the furnace door. Because the repair material depends on the residual temperature in the furnace to sinter, the faster the furnace is repaired, the less heat loss in the furnace, the higher the temperature, and the better the sintering. After the steel is discharged, the furnace door and the tapping port are easily cooled by the cold air. The slope of the tapping port is related to whether the molten steel can be poured out (if the molten steel cannot be poured out, the furnace bottom is easy to be damaged, and the chemical composition of the next furnace is easy to be unstable), so the two sides of the furnace door and the tapping port should be repaired first. In order to avoid the furnace slope holding line being stuck by the residue, you can also use an iron rake to scrape it before repairing the furnace. The other parts are relatively difficult to cool down. You can wait until the two sides of the furnace door and the tapping port are repaired before repairing. For the slag line and the furnace slope near the three-phase electrode, due to the effect of the electric arc, there is more erosion, so you should also pay attention to careful repair. It should be repaired thinly, because if it is repaired too thickly at once, the inner layer of magnesia sand is poorly heated and cannot be sintered well, resulting in large pieces of magnesia sand floating up during the smelting process and slag stickiness, so the thickness of the furnace repair is generally not more than 25mm. When the amount of furnace repair is large, some lime can also be added to the dolomite magnesia sand to further protect the furnace body. The furnace repair time depends on the erosion situation and the capacity of the furnace, generally 5min.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information