lmm@magnesiacarbonbricklmm.com

Technical support and construction service team

How to improve the service life of ladle slide bricks?

The corrosion of ladle slides has seriously affected the realization of multi-furnace continuous casting process. The technicians proposed to optimize the material of ladle slide bricks to improve the performance of the slide and adjust the casting process to ensure the multi-furnace casting of slide bricks. It is mainly reflected in the following aspects.

01 New R&D direction

Introducing a variety of metal powders and special nano-additives and graphitizing the carbon source to improve the bonding system of the slide, so that this metal-ceramic bonded non-fired and non-immersed slide has higher low-temperature strength, medium-temperature strength and high-temperature strength. Beijing University of Science and Technology applied the idea of ​​metal transition phase to refractory materials and studied metal transition phase composite refractory materials. It is believed that metal only plays a transitional role, gradually reacts with other raw materials during the material preparation process to form a good matrix, and is tightly compounded with particles.

02 Optimize the performance of ladle slide bricks

Use dense fused corundum as the main raw material, reduce the amount of SiO2 introduced in the raw material, improve the purity and corrosion resistance of slide bricks; add appropriate carbon-containing raw materials to improve the thermal shock stability of slide bricks; add reinforcing agents to the matrix, and form a ceramic bonding phase of SiC whiskers during the firing process to improve the hot strength of the slide bricks, while preventing the expansion of cracks to further enhance the thermal shock stability; require suppliers to improve the processing flatness and finish of the sliding surface, and apply lubricants on the sliding surface to reduce resistance during sliding and prevent oxygen absorption and oxidation during pouring. At present, the physical and chemical indicators of slide bricks used in Shougang Jingtang Ladle are shown in Table 1.

w(Al₂Os)%w(ZrO₂)%w(FC)%Bulk density/(g ·cm-3)Apparent porosity/%Normal temperature compressive strength/MPaHigh temperature flexural strength/MPa
>74  >4≥7≥3.1≤8≥130 >40
slide gate plate nozzle

03 Usage requirements

Shougang Jingtang requires that the surface of the slides used in 2 to 4 furnaces should not have refractory material falling off or sticking, no steel sandwiching between the slides, no obvious cracks on the slide surface, no “V”-shaped melting loss or enlarged aperture of the steel casting holes. Focus on observing whether there is slag intrusion in the cracks around the aperture, whether the cracks are open, and whether the crack surface is accompanied by oxidation and particle peeling. If the above phenomena exist, the slide should be replaced immediately; if fine cracks are found and the surface around the cracks is flat, the cracks are normal cooling cracks and the slide can continue to be used; sometimes fine cross cracks can be seen on the upper plate surface in the closed position of the lower slide, which is normal and the slide can continue to be used; if obvious horizontal and vertical cross cracks are found in the direction of the slide, the slide should be replaced. When a “step” appears at the joint of the upper slide and the upper water inlet after use, aluminum-chromium fire clay must be used to bore the hole. Before boring, the residual material in the water inlet eye must be blown clean with an air duct, and then the fire clay is used to eliminate the “step”. When boring, the mud material must be evenly, smoothly, firmly, and of appropriate thickness. The hole diameter of the upper water inlet brick after boring is not less than 85mm. In production practice, it is strictly forbidden to use slides with water inlet hole erosion and expansion greater than 10mm. If the width of the water inlet crack is greater than 1mm or the crack width is not greater than 1mm but there are 2 or more cracks, or ring cracks are found, the water inlet must be replaced.

Ladle slide gate plate

04 Results and analysis

After the research and development of Shougang Jingtang technicians, under the premise of ensuring safe use, the service life of Shougang Jingtang ladle slides has been significantly improved, and the service life of the ladle slides has been increased from an average of 2.8 furnaces to the current 3.6 furnaces. The increase in the number of furnaces used for the slide plate not only reduces the production cost, but also reduces the labor intensity of the ladle hot repair workers. After the slide plate was used for 4 furnaces, the slide plate surface and the steel pouring hole were eroded evenly without obvious cracks. The slide plate used for 4 furnaces was used on site. The surface was flat and smooth, the slideway had no obvious roughening phenomenon, the pouring hole had no expansion and corrosion phenomenon, and no obvious large cracks occurred around the hole diameter.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information