lmm@magnesiacarbonbricklmm.com

Technical support and construction service team

LF Ladle Furnace Argon Blowing and Inclusion Removal

The factors affecting the removal of inclusions by argon blowing during the refining process of the ladle furnace are analyzed, the relationship between the two is discussed, and suggestions are put forward for the bottom argon blowing system of the ladle furnace.

1 Introduction

With the technological progress of the steel industry, a wide variety of off-furnace treatment technologies have emerged and have become an indispensable supporting means in steelmaking production. Due to its simple equipment, low investment, flexible operation and good refining effect, the LF ladle refining furnace has become the main refining equipment in the metallurgical industry and has been widely used and developed at home and abroad. Argon blowing and stirring is one of the important refining methods of the ladle furnace. Bottom argon blowing can even out the composition and temperature of the molten steel. The most important function is to promote the removal of inclusions in the molten steel. Starting from the basic principle of removing inclusions by blowing argon in the ladle furnace, this paper analyzes the factors affecting the removal of inclusions when blowing argon in the ladle furnace and the effective means to improve the efficiency of removing inclusions.

2 Principle and analysis of influencing factors

2.1 Principle of argon blowing to remove inclusions

The removal of inclusions in molten steel under argon blowing from the bottom of the ladle mainly relies on the flotation effect of bubbles, that is, the inclusions collide with bubbles and adhere to the bubble wall, and are removed as the bubbles float up. The process of inclusion particles being captured by bubbles is shown in Figure 1, which can be decomposed into 5 steps: (1) Inclusions approach bubbles and collide. (2) A steel liquid film is formed between inclusions and bubbles. (3) Inclusions slide on the bubble surface. (4) Dynamic three-phase contact is formed to remove and rupture the liquid film. (5) Stabilization and floating of inclusions and bubble clusters. In the 5 steps, the collision of inclusion particles with bubbles plays a core role.

2.2 Analysis of factors affecting argon blowing to remove inclusions

2.2.1 Stirring power

The main tasks of early refining are to uniform the temperature of molten steel and promote mass transfer, i.e. desulfurization. In order to ensure sufficient desulfurization during the refining process, argon blowing at the bottom of the ladle must use as little argon as possible to generate the maximum stirring energy and the shortest uniform mixing time. This inevitably forms slag rolls. When the air blowing is increased to a certain extent, the liquid surface is violently disturbed, the flow velocity of the slag interface increases, and two standing waves are formed at the liquid surface. At the trough of the standing wave, the liquid slag layer is sheared by the molten steel descending from the wave crest, and is drawn into the molten steel flow field to pollute the molten steel. The schematic diagram of the pollution process is shown in Figure 2.

2.2.2 Number of air bricks

In determining the number of air bricks, although we recognize the advantages of double air bricks in removing inclusions, in ladles with a capacity of less than 100 t, the use of double air bricks for argon blowing actually aggravates slag rolling.

2.2.3 Argon flow rate

Argon blowing to remove impurities runs through the entire refining process. Excessive argon flow rate aggravates slag rolling and reduces the probability of capturing impurities; too small argon flow rate cannot provide sufficient stirring energy and the total amount of bubbles blown. It is necessary to determine a reasonable argon flow rate to meet the requirements of molten steel refining. Large particle inclusions are easily captured by bubbles, while small bubbles are more conducive to capturing inclusions than large bubbles. Using high-intensity argon blowing can only coarsen the bubbles but cannot achieve the purpose of effectively removing inclusions. Figure 3 shows the behavior of bubbles under different argon flow rates. As shown in Figure 3, when the argon flow rate is small, the bubbles generated are dispersed bubble groups. As the argon flow rate increases, the bubbles begin to gather to form bubble bags.

2.2.4 Soft Blowing

The inclusion removal efficiency during the soft blowing period depends on the apparent argon flow rate at the outlet of the permeable brick and the total amount of argon blown into the molten steel, the latter also represents the total number of bubbles blown into the molten steel. (1) Increasing the argon blowing flow rate increases the apparent flow rate at the outlet of the permeable brick, increases the bubble detachment size, and reduces the probability of bubbles capturing inclusions; but increasing the argon blowing flow rate also means that the number of bubbles blown into the molten steel per unit time increases. From this point of view: ① Large inclusions are easier to remove than small inclusions; ② Small permeable brick aperture is conducive to reducing the bubble detachment size, which is conducive to inclusion removal; ③ Small argon blowing flow rate is conducive to reducing bubble size and increasing the probability of bubbles colliding with inclusions, but the inclusion removal efficiency ultimately depends on the total amount of bubbles blown into the molten steel. Reducing the argon blowing flow rate must extend the argon blowing time, which is often limited by the production process; ④ Increasing the area of ​​the permeable brick and selecting a small permeable brick aperture are very effective in improving the inclusion removal efficiency. The number of argon bubbles blown into the molten steel can be doubled within a limited refining time, greatly improving the removal efficiency of inclusions. (2) Select a reasonable soft blowing argon flow rate to ensure that secondary slag roll-off does not occur. At present, in actual production, the soft blowing flow rate is usually set at a limit that does not blow out the “naked eye”. However, from the perspective of improving the efficiency of removing inclusions from the molten steel, the upper limit of the argon blowing flow rate determined by this method may be too large, and individual furnaces with thick slag layers will aggravate slag roll-off.

2.2.5 Argon blowing device

It should be able to accurately and timely adjust the argon flow rate to meet various refining process requirements. Although the existing argon blowing device has undergone a major equipment transformation, the actual operation on site is still mainly manual. The human factors of the operator seriously affect the stability of continuous production, and there is no historical accumulation of argon flow values.

3 Suggestions

(1) Increasing the argon blowing flow rate can improve the stirring energy and shorten the uniform mixing time, which is beneficial to desulfurization. (2) Weak stirring of the ladle and appropriately extending the soft blowing time are more conducive to removing inclusion particles in the steel; for large ladles, double permeable bricks should be used reasonably to achieve the purpose of low stirring power and short refining time. (3) The efficiency of bottom blowing argon to remove inclusions in steel mainly depends on the argon bubbles and the amount of gas blown into the molten steel. The probability of small-diameter bubbles capturing inclusion particles is higher than that of large-diameter bubbles. Increasing the area of bottom-blown permeable bricks and selecting small permeable brick apertures can reduce the apparent flow rate of argon at the outlet of the permeable bricks, thereby reducing the detachment size of argon bubbles at the outlet of the permeable bricks and increasing the probability of bubbles capturing inclusions. (4) Select advanced and reasonable argon control devices to achieve accurate and timely automatic control of argon blowing, and summarize a reasonable argon blowing system suitable for your own situation through long-term data accumulation.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information