Magnesia carbon bricks are very suitable for the requirements of iron and steel smelting due to their superior high temperature resistance, slag erosion resistance, and good thermal shock stability. Taking advantage of the properties of carbon materials that are difficult to be wetted by slag and molten steel and magnesia, high slag resistance and solvent resistance, and low high temperature creep, magnesia carbon bricks are used in severely corroded slag lines and outlets. Steel mouth and other parts. So far, due to the extensive use of magnesia carbon bricks in the steelmaking process and the improvement of the steel smelting process, huge economic benefits have been created.
LMM GROUP uesd for MgO-C bricks instead of high alumina bricks to increase high using performance for Egypt customer Previously service life of high Al brick is 50 heats. But now, after designed and changed by LMM engi-neer, MgO-C brick finally achieved 86 heats operation. They are satisfied to our quality.

When MgO-C bricks are used in refining ladle furnaces and steel ladles, they are primarily applied in zones such as the freeboard and the slag line. Depending on the operating conditions, the refractories used in these areas must possess excellent high-temperature resistance, thermal shock resistance, and resistance to mechanical wear caused by slag attack. Therefore, magnesia-chrome refractories were used in these zones in the past. However, considering that chromium poses environmental pollution risks, their usage has decreased, and magnesia-carbon bricks are now the preferred choice.
Because the magnesia-carbon bricks in a new ladle can suffer severe degradation during the preheating process, the loose decarburized layer can reach a thickness of 30 to 60 mm. This zone is washed away during the teeming (pouring) of molten steel, carrying the magnesia grains into the slag. Obviously, preventing the carbon in the magnesia-carbon bricks from being oxidized during preheating has become one of the critical steps to improve the service life of the magnesia-carbon bricks in the freeboard and slag line zones of the ladle. In addition to adding composite antioxidants to the magnesia-carbon bricks, the key technical measure is to coat the surface of the bricks with an alkali-containing low-melting glass phase liquid after lining, so as to protect the carbon in the magnesia-carbon bricks from oxidation during the ladle preheating process.

Currently, almost all electric arc furnace (EAF) walls are lined with magnesia-carbon (MgO-C) bricks. Consequently, the service life of MgO-C bricks determines the campaign life of the furnace. The primary factors governing the quality of EAF MgO-C bricks include: the purity of the dead-burned/fused magnesia as the MgO source, the types of impurities, and the bonding state and size of the periclase grains; the purity, degree of crystallinity, and flake size of the flake graphite introduced as the carbon source; and the amount added and the fixed carbon (residual carbon) content of the thermosetting phenolic resin, which is typically selected as the binder. It has been proven that adding antioxidants to MgO-C bricks can modify and improve their matrix structure. However, under normal EAF operating conditions, antioxidants are not an essential raw material. Only in EAFs handling high-FeOn slag—such as those utilizing direct reduced iron (DRI), areas subjected to irregular oxidation, and hot spots of the furnace—does the addition of various metallic antioxidants become a critical component of the bricks.
The wear and erosion behavior of MgO-C bricks in the slag line is characterized by the formation of a distinct dense reaction layer and a loose decarburized layer. The dense reaction zone, also known as the slag penetration zone, is the eroded region where high-temperature liquid slag penetrates the brick body through the massive pores formed after decarburization. Within this region, FeOn in the slag is reduced to metallic iron; even the exsolution phases and intergranular Fe2O3 solid-dissolved in MgO are reduced to metallic iron. The depth of slag penetration into the brick is primarily determined by the thickness of the loose decarburized layer and typically terminates where the residual graphite remains. Under normal conditions, the decarburized layer in MgO-C bricks is relatively thin due to the presence of graphite.
There are two tapping methods for EAFs: spout tilting tapping and bottom tapping. When spout tilting tapping is employed, MgO-C bricks are generally not used; instead, Al2O3-based or ZrO2-based refractories with additions of non-oxides like C, SiC, and Si3N4 are selected. When bottom tapping is utilized, the taphole consists of external sleeve bricks and internal sleeve (inner tube) bricks. The EAF bottom taphole utilizes MgO-C tube bricks, with the bore diameter determined by factors such as furnace capacity and tapping time, generally ranging from 140 to 260 mm.
An EAF in a certain steel plant used medium-grade and low-grade MgO-C bricks at the taphole and on both sides of the taphole to replace the traditionally used sintered magnesia bricks, achieving excellent preliminary results. The furnace campaign life increased from around 60 heats to more than double. After service, the MgO-C bricks at the slag line remained relatively intact with no slag sticking. No furnace patching was required at the slag line, which reduced labor intensity while simultaneously improving molten steel purity and productivity.

Since the operating conditions vary across different parts of the converter working lining, the performance and service life of magnesia-carbon (MgO-C) bricks also differ.
(1) Furnace Mouth: Due to the drastic temperature fluctuations at the furnace mouth, the scouring effect of slag and high-temperature waste gas is quite severe. Furthermore, the mouth is subjected to impacts during scrap charging and addition operations. Therefore, the refractories used for the mouth must possess excellent thermal shock resistance and slag resistance; they must withstand the scouring of molten slag and high-temperature waste gas, resist steel sticking (skulling), and be easy to clean.
(2) Cone (Furnace Cap): The cone is a zone subjected to severe slag attack. It is simultaneously affected by temperature fluctuations, carbon oxidation, and the scouring of dust-laden waste gases. Consequently, magnesia-carbon (MgO-C) bricks with high slag resistance and strong thermal shock resistance are required.
(3) Charging Side: During blowing, the splashing of slag and molten steel easily causes chemical erosion, wear, and scouring on the charging side. Additionally, this side suffers direct impact and erosion from the charging of scrap and hot metal, leading to severe mechanical damage. Therefore, besides high slag resistance and exceptionally high hot strength, the MgO-C bricks must also possess excellent thermal shock resistance. High-strength MgO-C bricks with added antioxidants are typically adopted.
(4) Tapping Side: The tapping side is basically free from mechanical damage during charging, and the impact of thermal shock is also relatively small. However, it is subjected to the thermal shock and scouring of molten steel during tapping. Its wear rate is much lower than that of the charging side. When using the exact same material as the charging side, a thinner lining configuration than the charging side is adopted in masonry to maintain a balanced life of the converter lining (zoned lining).
(5) Slag Line Zone: The slag line is the zone where the lining is in long-term contact with the molten slag, resulting in severe slag attack. On the tapping side, this is often not prominent because the position of the slag changes with the tapping time. On the slag tapping (deslagging) side, wear is severe due to the intense slag attack combined with other effects that the belly zone undergoes during blowing. Therefore, the masonry of MgO-C bricks with outstanding slag resistance is required.
(6) Trunnion Areas: In addition to the damage during blowing, the surfaces of both trunnion areas are not covered by a protective layer and are difficult to repair. Consequently, the carbon in the lining material is easily oxidized, leading to severe degradation. High-grade MgO-C bricks with excellent slag resistance and strong oxidation resistance should be applied.
(7) Hearth and Bottom: These areas are subjected to the violent scouring of molten steel during blowing. However, compared with other zones, their degradation is generally lighter. MgO-C bricks with low carbon content or tar-dolomite bricks can be selected. When high-speed blowing is applied and the molten pool is shallow, the central area of the furnace bottom may suffer severe damage. In addition, when bottom blowing is employed, damage in these areas may intensify, and the same material as the charging side of the belly should be used.
Currently, to improve the technical and economic indicators of converters, combined lining (comprehensive masonry) is widely adopted.
By replacing high alumina bricks with optimized MgO-C bricks, users can significantly increase performance. For instance, LMM GROUP helped a client increase service life from 50 heats to 86 heats.
While both offer high resistance, magnesia-chrome refractories pose environmental pollution risks due to chromium. MgO-C bricks are an eco-friendly and high-performing alternative.
Zoned lining applies different grades or thicknesses of MgO-C bricks based on the specific wear rate of areas like the trunnions, slag line, and hearth to achieve a balanced and cost-effective furnace life.