The actual use volume of a company’s ladle seriously affects the production rhythm of the converter and also restricts the production efficiency of the 300t converter. The average furnace output of 300t converters at home and abroad should be greater than the nominal design capacity, while the average furnace output of the company’s 300t converter is less than 290t, which is an important bottleneck that has long plagued production efficiency. Therefore, the company is determined to tackle the problem of ladle capacity increase, thoroughly solve the various drawbacks caused by the ladle being too small, and achieve efficient and stable production operation.

Ladle capacity increase and expansion transformation

01 Requirements for ladle capacity increase transformation

In order to reduce the cost of transformation, the company decided to maximize the use of the existing cladding and reuse the ladle bottom, ladle bottom support, and tilting device. The ladle bottom maintains the existing dimensions of each part, the large supports around the trunnion seat and the ladle seat are reused, the welds and heat-affected zones with the cylinder are cut off, and 35mm is cut off on both sides. The length of the ear shaft embedded in the ear shaft seat is shortened accordingly, and the inner ear shaft fixing block and the protruding part are kept consistent with the original inner wall of the ladle. The size of the ladle tilting device remains unchanged for reuse. The bottom of the ladle is first cut along the weld, and the height of the bottom of the ladle is cut by 90mm. The welding position of the ladle wall and the bottom of the ladle is changed from being level with the inside of the ladle bottom to being level with the outside. The transition welding is performed, and the edges and corners R20mm are polished and smooth. The bottom of the ladle has formed a small step before the transformation and is now flush with the wall. The thickness of the permanent layer of the ladle can be guaranteed to be the same after the construction. After the ladle capacity is increased, the ladle body diameter increases by about 68mm, so the ladle body steel plate needs to be replaced. To ensure strength, the thickness of the steel plate is increased from the original 40mm to 42mm. The ladle trunnion and trunnion seat are the most critical parts for ladle hoisting.

The life of the company’s 37 existing ladles is more than 8 years, and the trunnion has been ground during the hoisting process. For safety reasons, the trunnion is replaced during the capacity increase and transformation. In order to ensure that the external dimensions of the ladle remain unchanged after the capacity increase, the waist hoop and tank seat are newly made after the design institute’s review and approval, and the inner dimensions are shortened, but the plate thickness is increased to ensure strength; the position and horizontal distance between the hinge seat of the ladle cover and the upper mouth of the ladle are reduced by 35mm. The diameter of the ladle cover is the same as the outer diameter of the ladle, and the hinge seat is manufactured and constructed according to the drawing.

02 Impact on other equipment

After the ladle capacity expansion and transformation, the increase in the size of the ladle shell has a certain impact on related equipment. When the company expanded the capacity of the ladle, it fully considered the key limiting links such as the 480t crane gantry hook, offline ladle baking, molten steel car, 480t cross-car, LF furnace, RH furnace, CAS furnace, ladle capping system and casting machine turntable, ensuring that the above main equipment is not changed and other auxiliary equipment is appropriately adjusted, so that the project has good operability.

① Impact of capacity expansion on gantry hook

The center distance of the 480t crane gantry hook is 5600mm. After the diameter of the ladle shell is increased, how to ensure the normal and safe lifting of the ladle without replacing the gantry hook is a problem that must be solved. In order to ensure the stability of the gantry hook, after strict verification, the ribs on both sides of the ladle are shortened in the width direction and the thickness of the steel plate is thickened, so as to ensure that the spacing between the gantry hooks remains unchanged. After the ladle capacity is increased, each ladle of molten steel increases from the original 290t to the current 320t, the cladding weight is about 71t, the refractory weight is about 80t, the total weight is about 470t, and the overhead crane bears 480t, so the overhead crane load is not exceeded after the capacity increase.

② Impact of capacity expansion on ladle tire

After the ladle capacity is increased, the ladle diameter increases by about 68mm, so the original ladle tire used for knotting permanent layer needs to be scrapped, and the ladle tire diameter increases accordingly and matches the newly increased capacity ladle, and the size and structure of other parts remain unchanged.

③ Impact of capacity expansion on ladle-related auxiliary equipment

The height of the increased capacity ladle has not increased, so it has no impact on the ladle offline baking, LF furnace, RH furnace, and CAS furnace, but the thickening of the ladle will affect the ladle cover, the ladle support of the molten steel car seat, and the fork arm of the large ladle turntable. In order to avoid changing the current equipment size as much as possible, the equipment professionals finally reached a consensus through on-site surveying and mapping tests: the diameter of the new ladle mouth is 4700mm, which is equivalent to the diameter of the ladle cover. In order to prevent the ladle cover from falling into the ladle, it is required to install the ladle cover after the permanent layer is laid and the refractory bricks are laid. The diameter of the expanded ladle seat becomes 4386mm. After the ladle is seated in the molten steel car and the large ladle fork arm, the spacing on both sides is reduced from the original 35mm to the current 10mm. The reduced spacing has a certain impact on the stable seating of the ladle in the large ladle turntable. It is decided to grind and thin the ladle frame of the molten steel car seat and the wear-resistant belt of the large ladle fork arm by 15mm. At the same time, the manufacturer is required to control the diameter of the ladle according to the negative tolerance when making the ladle.

03 Requirements for masonry of expanded ladle

Before the permanent layer of the ladle wall is tied, ceramic fiberboard is laid on the ladle wall, and lightweight castables are used for knotting. The amount of water added to the lightweight material is controlled at about 6% to 8%, stirred evenly, and the new ladle mold is placed, and operated according to the existing process requirements. The bottom of the ladle is knotted with heavy materials, and the existing masonry method is still used for the bottom and nozzle seat bricks, that is, the upper and lower seat bricks are installed first, and then the bottom bricks are assembled. The gap between bricks should be less than 2mm, so that the brick joints are staggered vertically and horizontally, the brick joints are full of mud, and the bottom of the ladle is aligned and locked. For the ladle shell of the expanded and renovated ladle, the working layer of the ladle wall uses 190mm lining bricks and the slag line uses 210mm magnesia carbon bricks. Before the formal implementation of the ladle recovery capacity production organization, it must be guaranteed to be used more than 25 times. The working layer of the ladle wall of the medium repair ladle uses 180mm lining bricks and the slag line uses 210mm magnesia carbon bricks.

Ladle bottom blowing optimization

01 Optimize the structure of air-permeable bricks

During the use and pouring process of the original slit air-permeable bricks, high-temperature molten steel and slag may penetrate into the bottom-blowing air-permeable bricks through the gaps, causing the airway to be blocked by the infiltrated steel and slag. Therefore, a new type of slit composite diffused air-permeable brick was specially designed and manufactured, as shown in Figure 1.

The air-permeable brick mainly includes an argon rigid tube, a brick core body, a truncated cone (slit block), a dispersion block, and a brick core seat brick. The argon rigid tube is welded to the iron sheet of the brick core body, the truncated cone (slit block) is installed at the lower part of the inner part of the brick core body, the dispersion block is installed at the upper part of the inner truncated cone (slit block) of the brick core body, and the brick core seat brick is at the outermost side, wrapping the upper part of the argon rigid tube and the brick core body. Figure 1 After the slit-dispersion composite air-permeable brick was tested and promoted, it was found that this composite bottom-blowing brick can meet the current normal use, and the air permeability has been improved from 99.72% and stabilized at more than 99.85%, ensuring the bottom blowing effect of the ladle.

02 Improve the material of air-permeable bricks and increase the life of air-permeable bricks

The original bottom-blowing air-permeable bricks are mainly composed of plate-shaped corundum, spinel and chromium oxide. In actual use, it is found that their thermal shock stability and compressive strength are not high, and they may deteriorate under the hot pressure of molten steel, affecting their life and blowing rate. Therefore, the introduction of aluminum-magnesium spinel and chrome corundum can form micro cracks in the air-permeable bricks under the alternating hot and cold environment, buffer the thermal stress caused by temperature changes, reduce its peeling, and improve thermal shock resistance. In addition, considering that the company’s ladle is a large 300t ladle with an effective height of 4m for holding molten steel, the compressive strength of the bottom-blown air-permeable bricks must be enhanced, so the content of alumina powder is appropriately adjusted. The improved material of the air-permeable bricks is mainly composed of about 80% corundum, alumina powder, about 2.5% chromium oxide and magnesium-aluminum spinel, and about 3% binder is added.

During dephosphorization furnace steelmaking, if the life of the ladle bottom-blowing bricks is more than 15 furnaces, in order to ensure the bottom-blowing success rate, after burning the bottom blowing and putting the drainage sand, 10kg of drainage sand is put into the grooves of the bottom-blowing bricks on the east and west sides. Observe the residual thickness of the air-permeable bricks after unpacking at any time, and make the maximum use of the bottom-blowing air-permeable bricks under the premise of safe use to increase their service life. When the life of the bottom-blowing brick is ≥20 furnaces or it is found that the bottom-blowing brick is seriously eroded, special tools are used to measure the erosion depth of the bottom-blowing brick according to the size of different tilting machines. When the erosion depth is ≥280mm, the ladle must be dumped. The above measures increase the average service life of the ladle bottom-blowing brick from 23 furnaces to 25 furnaces, and the average ladle repair age is also significantly improved.

03 Optimize the purge device

After the ladle cover project is fully put into use, the ladle lining temperature can reach more than 1300℃, and the ordinary oxygen-burning pipe will bend after entering the ladle, which greatly increases the difficulty of purge. The inability to effectively purge the ladle bottom-blowing brick will cause insufficient air permeability of the bottom-blowing brick, resulting in a significant increase in the number of abnormal refining bottom blowing furnaces. To solve this problem, the purge device was improved. The device adopts an inner tube and an outer tube connected by a retaining ring, a gas pipe is welded to the outer tube and connected to the outer tube, a handle is welded to the outer wall of the outer tube, and a gas channel is provided between the outer tube and the inner tube, which can ensure the rapid purging of the bottom blowing bricks of the covered ladle and avoid the reduction of the service life of the bottom blowing bricks due to excessive purging of the bottom blowing bricks when purging with an oxygen-burning tube.

04 Optimize bottom blowing process

In order to avoid the influence of air leakage in the automatic bottom blowing pipeline on the bottom blowing, the automatic bottom blowing pipeline of the ladle is changed from coming out from the female end of the mushroom head of the ladle and then entering the bottom of the ladle downwards to connecting with the hand-inserted pipe. After coming out from the mushroom head, it goes up along the ladle wall through the ladle reinforcement hole and connects with the hand-inserted pipe on the left side of the hand-inserted pipe. When the automatic bottom blowing pipeline of the ladle is not used or there is air leakage at the bottom blowing mushroom head of the automatic bottom blowing pipeline, the valve of the automatic bottom blowing pipeline is closed and the hand-inserted pipe is used for bottom blowing. The method for checking air leakage in the back-blowing pipeline of the ladle bottom blowing brick is as follows: first close the argon pressure reducing valve, open the main argon valve, and observe the flow display. If the display shows within 50L/min, it means that there is no air leakage in the pipeline. If the number is greater than 50L/min, it means that there may be air leakage in the back-blowing pipeline and joints, which needs to be checked and handled in time. After the implementation of the above four measures to optimize the bottom blowing process, the blowing rate of the ladle has been significantly improved.

The annual average success rate of bottom blowing increased from 99.84% and stabilized at more than 99.98%. The average service life of ladle bottom blowing bricks increased from 23 furnaces to 25 furnaces, and 5 sets of ladle abnormal offline due to bottom blowing bricks were reduced every month. The technical and economic indicators have reached the level of advanced steel plants.

Application effect

After the company’s expanded ladle was put into operation, the quality of molten steel loading increased from the original 290t to the current 310t, which directly laid the foundation for the stable and high production of the steelmaking department. The annual production capacity of the first steelmaking converter increased by 7%, about 630,000 tons, and the total annual production capacity reached 9.7 million tons, close to the production level of Pohang Gwangyang. The expansion and transformation of the ladle effectively promoted the increase in steelmaking output, thereby effectively reducing the impact of the single furnace auxiliary on the output. At the same time, due to the increase in the output of a single furnace, the power cost, refractory cost and labor cost per ton of steel were reduced accordingly, greatly reducing the production cost per ton of steel. At the same time, the use of narrow-slit composite diffused air bricks at the bottom of the ladle, new coal oxygen guns and improvements in the bottom blowing process have increased the blowing rate from 99.84% to more than 99.98%. At the same time, the life of the bottom blowing bricks has also been significantly improved, reaching the level of advanced steel mills.

FAQ

What risks arise from the thinner refractory material after ladle expansion?

The most significant risk is a decrease in safety performance. Due to the thinner working or permanent layer, the cladding temperature will rise, easily leading to cladding deformation, weld cracking, and even steel leakage. Therefore, higher-performance refractory materials and optimized construction techniques must be selected.

What are the special requirements for refractory materials in the “slag line zone” after expansion?

The slag line area is most severely affected by slag erosion and thermal shock. After expansion, the molten steel level rises, necessitating a readjustment of the magnesia-carbon brick (MgO-C) arrangement. High-grade magnesia-carbon bricks with optimized carbon content and stronger erosion resistance should be selected to cope with liquid level fluctuations and high-temperature erosion.

Why must the “bottom-blowing process” be optimized after expansion?

Because the ladle volume increases and the liquid level rises, the original bottom-blowing pressure and flow rate may not meet the requirements for deep mixing. Without optimization, this can lead to uneven steel temperature, component segregation, or incomplete slag-metal reaction.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information