Products we offer
The Purging Plug is an important functional refractory component in the continuous casting machine, and plays a key role in the continuous casting production process. The following is a detailed introduction to the structure, working principle, function, performance requirements, common types, maintenance and replacement of the Purging Plug:
It is generally composed of a breathable material and an external sheath. The breathable material is usually a refractory material with a certain porosity and permeability. It is the core part of realizing the breathable function; the external sheath plays the role of protecting the breathable material, enhancing the overall structural strength and facilitating installation. It is generally made of metal material.Purging Plug
During the continuous casting process, an inert gas (such as argon) is introduced into the breathable plug, and the gas enters the molten steel evenly through the pores of the breathable material. This process utilizes the special microstructure of the breathable material. The tiny pores inside allow gas to pass through, but can effectively prevent the intrusion of molten steel.
Preventing nozzle blockage: During the continuous casting process, some inclusions in the molten steel tend to gather at the nozzle, causing nozzle blockage and affecting the normal casting. Blowing argon into the molten steel can effectively prevent inclusions from accumulating near the nozzle and ensure the smooth flow of the molten steel.
Removing inclusions: The blown argon forms a large number of tiny bubbles in the molten steel. These bubbles will absorb the inclusions in the molten steel during the rising process and bring them to the slag on the surface of the molten steel, thereby purifying the molten steel and improving the quality of the steel.
Uniform molten steel composition and temperature: The stirring effect of the gas makes the flow of molten steel in the crystallizer more uniform, which helps to eliminate the unevenness of molten steel temperature and composition, avoid local overheating or composition segregation, and improve the quality and performance of the ingot.
Good permeability: The permeable plug must have appropriate permeability to ensure that the gas can enter the molten steel evenly and stably. Too high permeability may cause molten steel to splash; too low permeability will not achieve the expected stirring and purification effect.
High refractory: Working for a long time in a high-temperature molten steel environment, the permeable plug needs to have excellent refractory properties and be able to withstand high temperatures without melting, deformation or damage.
Corrosion resistance: Molten steel contains various chemical components that will corrode the vent plug. Therefore, the vent plug should have good erosion resistance to ensure its service life and working stability.
Thermal shock stability: During the continuous casting process, the vent plug will experience frequent temperature changes, which requires it to have good thermal shock stability and be able to resist rapid temperature changes without cracking or peeling.
Dispersed vent plug: The internal pore distribution of the permeable material of this vent plug is relatively diffuse, and the gas enters the molten steel evenly through many tiny pores, with a good stirring effect, which can effectively remove inclusions and is suitable for occasions with high requirements for molten steel quality.
Directional vent plug: Its internal pores have a certain directionality, and the gas enters the molten steel along a specific direction, which can form a strong local stirring effect. The gas flow direction and stirring area can be adjusted according to different continuous casting processes and requirements.
Daily inspection: Regularly inspect the appearance of the vent plug to check whether there is damage, erosion, blockage, etc. At the same time, monitor the permeability and gas flow of the vent plug to ensure that it works properly.
Cleaning and maintenance: During the continuous casting process, some steel slag and impurities may adhere to the surface of the vent plug, which needs to be cleaned in time to ensure the air permeability. Care should be taken to avoid damaging the air permeable material during cleaning.
Replace in time: When the vent plug is severely damaged, the air permeability cannot meet the process requirements or reaches the end of its service life, it should be replaced in time to ensure the smooth progress of continuous casting production and the quality of the ingot.
LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.
Trusted by Global Steel Leaders