lmm@magnesiacarbonbricklmm.com

Technical support and construction service team

Production practice of reducing converter steel consumption

[Abstract] This paper analyzes various factors that affect converter steel consumption in the steelmaking process, and proposes some new measures to reduce converter steel consumption.

[Keywords] Converter; Steel consumption; Measures

Introduction As we all know, the steel consumption in the converter smelting process accounts for more than 83% of the total steel consumption, so reducing converter steel consumption is one of the effective means for enterprises to reduce costs. Under the current severe situation, the raw materials used in the steelmaking process are diversified and the composition is unstable, resulting in large fluctuations in converter steel consumption in recent years. In order to further reduce the consumption of converter steel, by exploring the best loading mode, improving the converter raw material structure and furnace smelting process, adopting the less slag steelmaking process, reducing splashing, reducing blowing loss, reducing slag strip steel and other measures, the steel consumption has been reduced from the original 1081.6Kg/t to the current 1072.3Kg/t.

1 Main factors affecting the consumption of steel materials in converter smelting

1.1 Overview of the consumption of steel materials in converter smelting

The main factors affecting the consumption of steel materials include chemical loss of impurity elements in raw materials, smoke loss, metal loss in slag, iron loss caused by splashing and slag strip, etc. In order to reduce the blow loss of converter and reduce the consumption of steel materials, a reasonable raw material structure, appropriate loading system and appropriate slag making process should be adopted and stabilized converter operation to achieve.

2 Measures to reduce the consumption of steel materials in the converter

2.1 Optimize the ratio of raw materials entering the furnace

According to the conditions of the molten iron, the ratio of molten iron to scrap steel should be appropriately increased to make the converter heat slightly surplus. Within the appropriate dosage range, by using washed slag steel and granular scrap steel to replace part of the iron blocks, increasing the amount of magnetic slag steel and reasonably controlling the amount of ore, the amount of molten steel can be effectively increased, thereby reducing the consumption of steel materials. In actual production, due to the high SiO2 content in washed slag steel, even if the total amount of slag-making materials added is the same, the amount of slag produced by using washed slag steel is also large, resulting in a high iron consumption in the slag. The price of granular scrap steel is relatively cheap, so it can be used in moderation. Magnetic slag steel is magnetically selected from the bottom slag of the furnace, which is self-produced and sold. At present, the monthly output of the steel plant is about 2,500 tons. The cooling and slag adjustment capabilities of magnetic slag steel are weaker than those of ore. In the converter smelting process, when the slag is more active or the process temperature is higher, it can be added appropriately. It can cool down without making the slag too active. Although the ore grade is high, the block size is appropriate, and the Fe recovery rate is high, the economic benefits are not suitable compared with self-produced magnetic slag steel and water-washed slag steel through statistical calculation and cost analysis. In order to maximize the use of magnetic slag steel, improve the reduction effect of magnetic slag steel and reduce the impact of excessive addition of magnetic slag steel on smelting stability during blowing, the ore and magnetic slag steel addition smelting process was explored in actual production. According to the chemical reaction characteristics of ore and magnetic slag steel, the ratio of magnetic slag steel and ore is added in each batch of slag material before and during blowing at a ratio of 4:1. When the slag is too active in the middle of blowing, the gun position is adjusted and a small amount of magnetic slag steel is added in batches to avoid splashing caused by concentrated addition in the middle of blowing; it is strictly forbidden to add magnetic slag steel in the late stage of blowing to avoid the effect of strong slag oxidation on deoxidation and alloying caused by the late addition of magnetic slag steel, which will cause the molten steel to return to phosphorus and the poor melting reduction effect.

2.2 Optimize slag making process and reduce slag iron consumption

Reduce the FeO content and metal droplet content in the final slag: increase the bottom blowing gas flow rate in the later stage of blowing to reduce carbon oxygen accumulation, so as to reduce the oxygen content in the steel and make the molten pool stirring more fully and steadily. In order to reduce the FeO and metal droplet content in the final slag, low-position high oxygen pressure measures are adopted at the end in actual production, and the hit rate of carbon pulling is strictly controlled in one time to increase the carbon content at the end. At the same time, measures such as strictly prohibiting the addition of ore and magnetic separation slag steel cooling in the later stage of blowing are also taken.

2.3 Control the final slag amount and implement low-slag steelmaking

In order to reduce the slag production of a single furnace, the low-slag steelmaking process is promoted on the basis of further improving the converter slag operation process. In terms of raw materials, high-grade lime is used, and light-burned dolomite is used instead of raw dolomite for slag making as much as possible to reduce the amount of iron blocks in scrap steel. The molten iron adopts the “three-removal” treatment process, and the molten iron after treatment must be cleaned of the slag.

2.4 Improve the blowing process and reduce splashing losses

The following measures have been taken to eliminate or reduce splashing:

(1) Rationally control the amount of converter loading and the amount of slag-making materials used, and adopt a phased quantitative loading method according to the furnace age and furnace lining conditions.

(2) Improve the slagging process to ensure good slagging in the early stage. Before and after the addition of the second batch of slag-making materials, the peak of foam slag is moved forward by the method of early slagging so as to stagger the peak time of decarburization.

(3) Before the peak of decarburization arrives, appropriately increase the oxygen lance position and add magnetic separation slag steel and ore in small batches. According to the slag throwing situation at the furnace mouth, the lance position is then slowly lowered.

(4) At the end of blowing, high oxygen pressure and low lance position operation are adopted to increase the bottom blowing flow of the converter and strengthen the stirring of the molten pool. Especially in the later stage of furnace age, the stirring time at the low lance position should be appropriately extended to ensure the uniformity of the final molten steel composition and temperature, while reducing the oxidizability of the slag.

3 Conclusion

1) Strengthen the magnetic separation recovery of steel slag under the furnace and entering the slag field, recycle scrap steel as much as possible, and improve the recovery and utilization rate of self-produced magnetic separation slag steel and water-washed slag steel.

2) By reasonably improving the loading system, the converter operation is stabilized, the quality of blowing slag is improved, and the oxidation of the final molten steel is reasonably controlled, which can effectively reduce the iron loss caused by splashing and slag.

3) By reasonably adopting the types and structures of cold materials such as magnetic separation slag steel, and utilizing the slag-removing effect of cold materials such as magnetic separation slag steel and the price advantage over molten iron and scrap steel, the consumption of converter steel materials can be effectively reduced, the metal recovery rate can be increased, and the production cost can be reduced.

4) By reasonably controlling the composition of molten iron entering the furnace, reducing the amount of slag-making materials in the converter smelting process, further reducing the amount of converter slag, and implementing the low-slag steelmaking process, the slag iron consumption can be effectively reduced and the metal recovery rate can be increased.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time

Facebook
LinkedIn
Pinterest
Reddit

Comprehensive solution of Refractory for steelmaking

Fill out the form below, and we will be in touch shortly.
Contact Information