Requirements and configuration of refractory materials for VOD furnace

The VOD furnace is a device for oxygen blowing and decarburization under vacuum conditions outside the furnace. It is mainly used for secondary refining of ultra-pure, ultra-low carbon stainless steel and alloys. Figure 1 is a schematic diagram of the VOD method device.

Requirements and configuration of refractory materials for VOD furnace

The equipment was first manufactured by the Witten Special Steel Plant in Germany in 1965. There are currently about 80 units in the world, and more than ten in my country. The equipment has the following characteristics: the steel produced is of high purity and low carbon and nitrogen content; it is suitable for producing ultra-pure stainless steel and alloys with extremely low C, N, and O content; but the equipment is complex, the smelting cost is high, the decarburization speed is slow, and the production efficiency is low. The VOD equipment is mainly composed of a ladle, a vacuum tank, a vacuum system, an oxygen blowing system, an argon blowing system, an automatic feeding system, a temperature measurement and sampling system, and process detection instruments. Among them, the refractory material part is the ladle. The ladle consists of a molten pool, a slag line, and a free space. Among them, the refractory material of the slag line is the most easily damaged. Other refractory materials used include air-permeable bricks and ladle covers.

01 Basic functions of VOD

The VOD method is a method for smelting stainless steel under vacuum conditions, and has the following typical metallurgical functions:

(1) Oxygen blowing decarburization. The decarburization rate in the high carbon zone has nothing to do with the carbon content in the steel and is determined by the oxygen supply. The decarburization rate in the low carbon zone decreases as the carbon content in the steel decreases.

(2) Decarburization and chromium preservation. The chromium recovery rate can be maintained at 98.5%~99.5%.

(3) Blowing oxygen to increase temperature. The heat release of the oxidation reaction of metals (silicon, manganese, chromium, iron, aluminum, etc.) is used to increase the temperature of the molten steel.

(4) Vacuum degassing. Blowing argon and maintaining a certain vacuum degree can accelerate the diffusion of gas in the molten steel, which is beneficial to degassing.

(5) Slag making, deoxidation, desulfurization, and removal of inclusions. Making reducing high-basicity slag is beneficial to deoxidation and desulfurization.

(6) Alloying. Adding alloys under vacuum conditions can increase the alloy recovery rate and accurately control the composition of molten steel.

02 Effect of VOD furnace refining process on refractory materials

VOD is a refining device for smelting stainless steel, ultra-low carbon steel and alloys with oxygen blowing decarburization under vacuum conditions. The effects on the refractory materials of the furnace lining during the refining process are mainly as follows:

(1) Vacuum and high temperature. When the VOD furnace is smelted under vacuum, the vacuum degree in the furnace is 66.66~133.32Pa, and the temperature in the furnace can reach above 1700℃.

(2) Alkalinity change. The alkalinity is 0.5~4, and the alkalinity of the slag changes greatly, which has a strong erosion effect on the furnace lining materials. In the early stage of smelting, low-alkalinity slag is used. In the later stage, in order to preserve chromium and remove sulfur, it is required to produce reducing high-alkalinity slag with an alkalinity of more than 4.

(3) Fast flow and circulation of molten steel. Due to the simultaneous injection of argon and oxygen, the gas stirring effect is strong, and the erosion and wear of the lining materials by the molten steel and slag are large.

(4) Severe thermal shock. The VOD furnace is an intermittent operation equipment, which is used 2~3 times a day, so the temperature changes greatly, the temperature of the refractory changes violently, and is greatly affected by thermal shock.

(5) Long high temperature action time. Due to the long smelting time, generally about 1h, the furnace lining materials are subjected to long-term vacuum and high temperature action.

03 Requirements for refractory materials in VOD furnace

According to the smelting process conditions of VOD furnaces, refractory materials should have the following characteristics:

(1) Good stability under high temperature vacuum conditions.

(2) Under high temperature operating conditions, refractory materials should have the ability to resist slag penetration and erosion.

(3) They should have good thermal shock resistance.

04 Refractory materials used in VOD furnace

The slag line of VOD furnaces uses magnesia-chrome bricks or magnesia-calcium bricks, the side walls generally use magnesia-chrome or magnesia-calcium bricks, and the bottom also uses magnesia-chrome and high-alumina bricks. In recent years, zirconium bricks have also been used for the bottom.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time