Six ways to improve the life of converter oxygen lances

Affected by the high temperature and high pressure working conditions of converter smelting, the converter oxygen lance is easily affected by the slag and molten steel flow in the furnace during the blowing process, which is prone to burnout, sticking and other unfavorable situations, resulting in the replacement of the oxygen lance offline. As an essential process part for converter smelting, the oxygen lance occupies an important proportion in the converter process cost. Therefore, how to further reduce the consumption of converter oxygen lances has become the focus of steel mills to reduce process costs.

oxygen lance
oxygen lance

Scientifically control the furnace bottom value and improve the overall assembly accuracy.

In order to accurately grasp the furnace bottom situation, the post personnel are required to measure the furnace bottom of the first furnace in each shift, and determine the gun position at each stage according to the furnace bottom value; when the furnace bottom value rises seriously, the opening and end gun positions should be raised by more than the furnace bottom rise value. If the shift blows for multiple consecutive furnaces and the final slag is sticky, use the production interval to measure the furnace bottom twice and re-determine the gun position to prevent the furnace bottom from rising and burning the gun. Strictly control the total loading volume as required to ensure that the total loading accuracy rate is above 85% to avoid gun burning and sticking caused by large fluctuations in loading volume.

Strictly perform slag retention ignition operations to reduce splashing and gun burning.

When performing slag retention ignition operations, the personnel on duty are required to strictly implement the requirements for high oxygen pressure oxygen ignition, which can quickly penetrate the thick slag layer. If ignition is found to be difficult, the oxygen pressure for opening the blow can be increased, nitrogen can be purged, or the furnace can be shaken back and forth to reduce the pressure, so as to prevent forced ignition from causing large splashing and gun burning.

Strengthen the “one tank to the end” operation control to help the converter to blow smoothly.

Organize temperature measurement and sampling analysis of each tank of molten iron to the end, so as to facilitate timely adjustment of the loading volume in front of the furnace and avoid high-temperature splashing in the early stage. At the same time, do a good job in dealing with abnormal molten iron composition and temperature, and put the molten iron that does not meet the one tank to the end conditions into the mixed iron furnace to provide stable conditions for blowing.

Optimize the oxygen lance position control to ensure smooth blowing process.

During the process, the gun position is adjusted in a small range according to the “softness and hardness” of the furnace mouth flame. When the C-O reaction in the furnace is intense, the flame becomes hard, the slag furnace becomes thicker, and the slag begins to dry, the gun is raised in time to ensure that the slag is melted thoroughly at one time; after the slag furnace is melted thoroughly, when the flame becomes soft and weak, the gun is lowered in time to prevent secondary drying. According to the furnace mouth flame, when there are signs of drying, the gun is appropriately raised to alleviate the reaction in the furnace or the slag is dried, until the gun is lowered to the terminal gun position.

Adhere to the principle of adding small amounts in multiple batches and control the timing of slag addition.

The first batch of slag is added after the oxygen lance is ignited steadily. When the oxygen gun is lowered to the open blowing position, the remaining slag is added batch by batch according to the molten iron conditions and the previous slag melting situation.

Control the quality of the oxygen lance nozzle and improve the assembly quality.

Timely spot check each batch of oxygen gun nozzles; strictly control the production of oxygen guns to reduce the consumption of oxygen guns due to oxygen gun equipment.

LMM YOTAI established in 2007. Our production technology comes from Japanese Yotai. As an experienced and international player in the refractories industry. We have succeeded in expanding both the breadth of its product range and the depth of its services. From raw material selection, refractory portofio & optimization, installation & services & recycle of used refractories on site to further reduce client’s Opex & Capex in refractory consumption per ton steel output, meanwhile improve product quality of client.

Our Product have been supplied to world’s top steel manufacturer Arcelormittal, TATA Steel, EZZ steel etc. We do OEM for Concast and Danieli for a long time