Four factors for the damage of refractory magnesia carbon bricks for ladle slag line

Description: In the final analysis, the damage factor of magnesia carbon brick, a refractory material for ladle slag line, is the oxidation of carbon, including gas phase oxidation, liquid phase oxidation, indirect oxidation, and the influence of pores. The detailed analysis is as follows: Keyword: magnesia carbon brick for ladle furnace Gas phase oxidation That […]