Electric arc furnace steelmaking, using scrap steel as raw material, possesses unique advantages. Research shows that compared to smelting iron from ore and then refining steel, using scrap steel directly for steelmaking requires less infrastructure investment, saves 60% on energy, 40% on water, reduces waste gas emissions by 86%, and reduces slag by 97%. Simultaneously, the development of direct reduction ironmaking has provided metallized pellets to replace most of the scrap steel for electric arc furnaces, thus promoting the development of electric arc furnace steelmaking. Current steelmaking electric arc furnaces are developing towards larger scale, ultra-high power, and automated control. With the development of electric arc furnace steelmaking technology, higher requirements will inevitably be placed on the refractory materials used, making the current status and development of refractory materials for steelmaking electric arc furnaces a focus of attention.
Main Types and Smelting Processes of Electric Arc Furnaces for Steelmaking
Broadly speaking, electric arc furnaces for steelmaking include electric arc furnaces, induction furnaces, electroslag furnaces, and electron beam furnaces. Electric arc steel typically refers to steel produced using a basic electric arc furnace; therefore, this article focuses on electric arc furnaces (EAF). Electric arc furnaces are classified into two types: direct current (DC-EAF) and alternating current (AC-EAF). DC-EAF furnaces are increasingly used and are developing rapidly because they reduce the amount of refractory materials used, are more energy-efficient, produce less noise, and halve the flicker. For DC-EAF furnaces, new technologies such as eccentric bottom tapping, water-cooled furnace walls, water-cooled furnace covers, oxygen-burner nozzles, and scrap preheating are suitable and effective.
DC-EAF furnaces have a graphite electrode at the furnace top, resulting in a stable and concentrated arc. This leads to good molten pool stirring and uniform temperature distribution within the furnace, improving melting efficiency. A typical characteristic of DC-EAF furnaces is that the graphite electrode at the furnace top serves as the cathode, with the anode connected to the furnace bottom. This requires the furnace bottom to be conductive. The main conductive materials available for the furnace bottom include: (1) conductive refractory materials (ABB); (2) metal components: including steel rod electrodes (Irsid-Clecim), steel sheet electrodes (VAI), multi-needle steel electrodes (GHH), and copper-steel composite water-cooled bottom electrodes. Except for the special requirements for the refractory materials used in the bottom of DC electric arc furnaces, the refractory materials used in other parts are very similar. The most widely used type of AC electric arc furnace (AC-EAF) is the ultra-high power electric arc furnace (UHP-EAF). This type of electric arc furnace has high production efficiency, slow furnace wall wear, and advantages such as shortened melting time, improved thermal efficiency, reduced power consumption, and stable arc.
Electric arc furnaces can be classified into trough-type tapping electric arc furnaces and eccentric bottom tapping electric arc furnaces (EBT) according to the tapping type. Because the eccentric bottom (EBT) tapping spout can expand the water-cooled area, reduce refractory material costs, and reduce the amount of slag discharged from the ladle, its application is gradually increasing. Electric arc furnace (EAF) steelmaking uses scrap steel and metallized pellets as raw materials. It primarily utilizes the heat of an electric arc to transform scrap steel into virgin steel through a series of metallurgical and chemical reactions at temperatures reaching up to 4000℃ in the arc zone. The smelting process is generally divided into melting, oxidation, and reduction phases. The furnace can create both oxidizing and reducing atmospheres, resulting in high efficiency in dephosphorization and desulfurization.In my country, EAF steelmaking mainly produces high-quality alloy steel. In recent years, with the continuous evolution of EAF steelmaking technology, including higher operating temperatures, larger furnace capacities, more rapid temperature changes, and increasingly demanding alloy steel quality requirements, higher demands have been placed on refractory materials.
Damage Mechanism of Refractory Materials Used in Electric Steelmaking Furnaces
Electric steelmaking furnaces typically operate in an alkaline corrosive atmosphere. Therefore, the refractory materials used in these furnaces are mostly basic refractories, such as MgO-C bricks, pitch-impregnated MgO bricks, MgO-Cr₂O₃ bricks, and MgO-CaO ramming mixes. A smaller portion consists of neutral refractories, such as Al₂O₃-C materials and high-alumina materials. Overall, the main damage factors affecting electric furnace refractory materials include: erosion, oxidation, scouring, melting, spalling, and hydration. Among these, oxidation, chemical corrosion, and scouring are the most dominant.
(1) Chemical Erosion: Acidic components in iron oxide (FeO) or slag, such as SiO₂, react chemically with CaO and MgO as follows:
FeO + MgO = FeO·MgO (1)
SiO₂ + 2MgO = 2MgO·SiO₂ (2)
CaO + SiO₂ + MgO = CaO·MgO·SiO₂ (3) All of these reactions can turn the furnace lining into molten slag, leading to the destruction of the refractory material.
(2) Oxidation: Oxidation is one of the main causes of refractory material erosion in electric furnace linings. During this process, the carbon components in the refractory material are oxidized by oxygen-containing components (such as iron oxide, oxygen, and magnesium oxide), leading to decarburization and damage to the material. FeO+C(s)=Fe+CO(g) (4)
O₂(g)+2C(s)=2CO(g) (5)
MgO(s)+C(s)=Mg(g)+CO(g) (6) The iron oxide in the slag reacts with the graphite or tar/resin on the hot side of the brick lining, or oxygen erodes the graphite or binder on the cold side of the brick lining. In both cases, the strength of the brick decreases, and it may be eroded by molten slag or steel.
Under the atmosphere of an actual electric furnace, reaction (6) is particularly easy to occur above 1700℃. The generated Mg vapor easily diffuses, causing structural deterioration, which is one of the main factors causing high-temperature damage to magnesia-carbon bricks.
(3) Erosion or Mechanical Impact
Physical damage is caused by the physical wear or erosion of the furnace lining due to the flow of molten steel or slag over the refractory material surface. Erosion is most common at the tapping spout, slag line, electrode port, or exhaust platform of the electric furnace. Spalling is a complex mechanism of refractory material damage. It is caused by the stress generated in the refractory material due to rapid heating and cooling of the furnace lining. This stress often exceeds the strength of the refractory material, leading to the intersection and penetration of cracks. Fragments of the furnace lining will spall off or completely detach, a common occurrence on the top of electric furnaces.
(4) Hydration
Hydration is also a factor contributing to the damage of electric furnace refractory materials. During use, water easily seeps into the furnace cover or walls. Water or steam can erode the refractory lining. Magnesium oxide (or other basic oxides) reacts with water (or steam) and becomes hydrated as follows:
MgO(s) + H₂O(l/g) = Mg(OH)₂(s) (7)Reaction (7) leads to a significant weakening of the refractory material’s performance, resulting in poor resistance to slag and molten steel penetration. Based on the above analysis of the causes of damage, it can be seen that the refractory materials selected for various parts of the steelmaking electric furnace have the following performance requirements: ① good chemical and volume stability; ② the material composition should not easily react with molten steel or SiO₂, and should not easily form nodules; ③ it should not be easily wetted or penetrated by molten steel; ④ it should have good resistance to rapid cooling and heating, and should not be easily damaged or peeled off; ⑤ it should have high density, low porosity, and uniform pore distribution, and should not be easily penetrated by molten steel; ⑥ it should have high strength and be able to resist mechanical impact and erosion.
Research and Application of Refractory Materials for Steelmaking Electric Furnaces
Table 1 lists the main refractory materials used in steelmaking electric furnaces in major countries and regions around the world, including furnace bottom electrodes, furnace bottom, furnace lining (metal wire), tapping system and furnace cover, etc.
| Furnace type and parts | Japan | China | North America | Europe | |
| DC–Clecim Furnace Type | Electrode sleeve brick | Magnesia-carbon bricks | Magnesia-carbon bricks | Magnesia-carbon bricks | Oil-impregnated and fired magnesia bricksMagnesium aluminum spinel partsMagnesium chrome bricks |
| Bottom of the furnace | Magnesium-calcium dry ramming mix | Magnesium-calcium dry ramming mix | Magnesium-calcium dry ramming mix | Magnesium-calcium dry ramming mix | |
| DC–ABB furnace type | electrode | Conductive magnesia-carbon bricks, conductive fire cement | Conductive magnesia-carbon bricks, conductive fire cement | Conductive magnesia-carbon bricks, conductive fire cement | Conductive magnesia-carbon bricks, conductive fire cement |
| Bottom of the furnace | Conductive ramming mix | Conductive ramming mix | Conductive ramming mix | Conductive ramming mix | |
| DC–GHH Furnace Type | Between steel needles | Magnesium-calcium dry ramming mix | Magnesium-calcium dry ramming mix | Magnesium-calcium dry ramming mix | Magnesium-calcium dry ramming mix |
| Bottom of the furnace | Conductive magnesia-carbon bricksConductive ramming mix | Conductive ramming mix | Conductive ramming mix | Conductive ramming mix | |
| UHP–EAF Furnace | Bottom of the furnace | Magnesia bricks, magnesia-carbon bricks, magnesia-calcium dry aggregate | Magnesia bricks, magnesia-carbon bricks, magnesia-calcium dry aggregate | Magnesia bricks, magnesia-carbon bricks, magnesia-calcium dry aggregate | Magnesia bricks, magnesia-carbon bricks, magnesia-calcium dry aggregate |
| furnace wall | side walls | asphalt-bonded magnesia-carbon bricks | asphalt-bonded magnesia-carbon bricks | asphalt-bonded magnesia-carbon bricks | asphalt-bonded magnesia-carbon bricks |
| Slag Line | resin-bonded magnesia-carbon bricks, magnesia-carbon sprayed aggregate | resin-bonded magnesia-carbon bricks, magnesia-carbon sprayed aggregate | resin-bonded magnesia-carbon bricks, magnesia-carbon sprayed aggregate | resin-bonded magnesia-carbon bricks, magnesia-carbon sprayed aggregate | |
| Permanent layer | fired magnesia bricks | fired magnesia bricks | fired magnesia bricks | fired magnesia bricks | |
| Steel tapping system | Steel tapping hole (base brick, sleeve brick) | magnesia bricks, magnesia-carbon bricks | magnesia bricks, magnesia-carbon bricks | magnesia bricks, magnesia-carbon bricks | magnesia bricks, magnesia-carbon bricks |
| Steel tapping trough | Magnesia-carbon bricks, Al2O3-MgO-C materials | Asphalt impregnation and firing of magnesia bricksMagnesium-carbon and alumina-carbon ramming mixes | Magnesia-carbon and alumina-carbon ramming mixes | Magnesia-carbon and alumina-carbon ramming mixes | |
| Stove lid | – | Magnesium-chrome bricksHigh-alumina castables | (Fired/Unfired) High-alumina bricks, corundum castables, magnesia-dolomite bricks | Magnesium-chrome bricksHigh-alumina castables | Magnesium-chrome bricksHigh-alumina castables |
Table 1 shows that the main types of refractory materials used in electric arc furnaces include: carbon-containing refractories, monolithic refractories, and non-fired products. Different parts of the electric arc furnace have different requirements for refractory materials. The requirements for refractory materials used in key parts (electrodes, working linings) are: ① high density, high-temperature structural stability, and wear resistance; ② non-wetting with molten steel and good slag corrosion resistance; ③ the material should preferably be alkaline or neutral. To meet the requirements of energy saving, long service life, low carbon emissions, and environmental protection, the refractory materials used in electric arc furnaces generally have the following characteristics: low carbonization, lightweight, chromium-free, and the use of monolithic refractories is increasing and developing rapidly.
1. Low Carbonization
Due to the development of clean steel and ultra-low carbon steel, as well as the requirements for energy saving and consumption reduction, the development of low-carbon refractory materials has become an inevitable trend. Currently, the main development trend of carbon-containing refractory materials used in various parts of the electric arc furnace, such as magnesia-carbon bricks, alumina-carbon materials, Al₂O₃-MgO-C materials, or other carbon-containing monolithic materials, is low carbonization and long service life. In recent years, with the development of preparation processes, the development of new binders, and the application of nano-carbon in refractory materials, it has become possible for carbon-containing refractory materials to develop towards low-carbon or even non-carbonized directions.
It is well known that the main problem caused by the reduction of carbon content in carbon-containing refractory materials is the decrease in thermal shock resistance and slag resistance. Currently, the main approaches to solving this problem include: ① Improving the thermal shock resistance of the material by improving the carbon structure of the bound carbon. Traditional binders for carbon-containing materials are mostly coal tar pitch or phenolic resin. After carbonization, the carbon structure of these binders is isotropic and glassy, making the material brittle, with a high elastic modulus, which is detrimental to the material’s thermal stability and also results in low high-temperature strength. Introducing graphitizable carbon precursors or catalytic oxides into coal tar pitch or phenolic resin allows these modified binders to carbonize into graphitized carbon or form nanofibers in situ under the product’s operating environment. This improvement in carbon structure and the reinforcing effect of nanofiber formation enhances the material’s thermal shock resistance and high-temperature strength. ② Optimizing the matrix structure of the material. With a significant reduction in carbon content, improving the contact ratio between aggregate particles and carbon particles—that is, reducing the size of carbon particles while ensuring their high dispersion—is a crucial measure to improve the thermal shock resistance and slag penetration resistance of low-carbon materials. Controlling the size, shape, and distribution of pores by adjusting the particle size distribution of the matrix also significantly affects the thermal conductivity of the material. ③ Employing highly efficient antioxidants. As the carbon content in the material decreases, protecting against carbon oxidation becomes particularly important; therefore, using suitable highly efficient antioxidants is essential.
The conductive refractory material used at the bottom anode of an ABB-type DC electric arc furnace determines the lifespan of the furnace bottom electrode. It must possess good conductivity, be insulated from the furnace shell, and ensure absolute safety. The most commonly used refractory material is MgO-C brick. MgO-C refractory materials are required to have the following characteristics: low and uniform resistivity with minimal temperature influence, low thermal conductivity, good high-temperature erosion resistance, and good high-temperature mechanical properties and wear resistance. To meet performance requirements, Japan initially used high-carbon MgO-C bricks, with carbon content reaching up to 25%, primarily in this area. Domestically, conductive MgO-C bricks with a carbon content of 18% are more commonly used.
“Hot spots” are prone to form near the electrodes in the electric arc furnace wall, accelerating the erosion and damage of the wall bricks and causing localized melting. This is a critical factor affecting the furnace’s lifespan. The refractory materials used in this area mainly include pitch-bonded high-purity magnesia bricks and magnesia-carbon bricks, with magnesia-carbon bricks being the most widely used. Research indicates that using high-purity magnesia raw materials and adding metal powder to promote densification can effectively improve the erosion resistance of MgO-C bricks.
Due to the widespread application of water cooling technology in the walls and lids of electric arc furnaces, water seepage or steam can cause hydration of MgO or magnesia-calcium materials, leading to material damage. Oil-impregnated magnesia bricks, pitch-impregnated magnesia bricks, or magnesia-calcium materials have become feasible measures to prevent hydration. The application of this new type of MgO brick in the permanent lining of electric arc furnaces effectively avoids hydration caused by water seepage or cooling system leaks during lining repairs, significantly extending the service life of the lining, reducing the frequency of permanent lining repairs and replacements, and effectively saving steelmaking costs.
The eccentric bottom taphole (EBT) is increasingly used due to its expanded water-cooled area, reduced refractory material costs, and decreased slag discharge from the ladle. EBT tapholes typically use EBT pipes surrounded by MgO-C bricks. With repeated tapping, the taphole erodes and its diameter increases, requiring replacement and maintenance, thus affecting the electric arc furnace’s production efficiency. While increasing the EBT pipe wall thickness to extend its service life initially can lead to low tapping efficiency due to the smaller inner diameter of the pipe.
2. Lightweighting
With increasing demands for energy conservation and environmental protection, lightweighting of kilns has become an inevitable trend. The development of low thermal conductivity energy-saving refractory materials mainly focuses on the following aspects: ① Using lightweight aggregates to design material structures, achieving lightweighting while ensuring the necessary erosion resistance, strength, and other functional properties; ② Microporous technology, adding loss on ignition to control the refinement and homogenization of pores; ③ Multi-layer gradient composite technology, researching the thermal matching stability control technology of the composite interface of structural refractory materials to prepare gradient lightweight refractory materials. A domestic refractory company has developed low-density fired magnesia bricks with a bulk density of 2.75–2.80 g/cm³ and an apparent porosity as high as 23%. These are mainly used as permanent linings for industrial kilns such as electric furnaces, possessing lightweight and heat-insulating properties, making them excellent energy-saving products. Their main components are: MgO 91.0%, CaO 2.5%, room temperature compressive strength ≥40 MPa, and softening temperature under 0.2 MPa load ≥1500℃.
3. Amorphous Refractories
The increasing variety of scrap steel used in electric arc furnace (EAF) steelmaking, especially the application of low-grade scrap steel, has made EAF operating conditions more demanding, accelerating the damage to refractory materials. To improve the service life of EAFs, higher requirements are placed on the refractory materials used in various parts of the furnace. The development of new amorphous refractories and the application of repair technologies have greatly advanced, significantly increasing the overall service life of the furnace lining without affecting normal production. Magnesia ramming mixes are mostly used in the working lining of the bottom layer of EAFs; however, due to direct contact with molten steel, this area is quickly damaged. Dolomite ramming mixes, with their excellent anti-stripping and wear resistance, have become a viable alternative, showing good application results.
For electrode lining bricks in DC electric arc furnaces, the extremely high temperatures during current flow and the erosion from molten steel and refining slag necessitate frequent repairs. Electrode lining brick repair is also achieved through thermal spraying, with a spraying temperature ≥800℃.
Conclusion
To meet the development needs of EAF steelmaking technology, a series of high-performance refractory materials have been developed and promoted for application both domestically and internationally. These refractory materials not only possess characteristics such as high-temperature structural stability, anti-sparging, wear resistance, and good slag resistance, but also embody the development concepts of energy conservation, emission reduction, and green environmental protection in the new era. With the rise of electric arc furnace steelmaking, refractory materials for electric arc furnaces will undoubtedly see even greater development.
The future development trends of refractory materials for electric arc furnaces in steelmaking are:
①Developing and promoting low-carbon (or carbon-free) and long-life refractory materials;
②Researching and developing lightweight refractory materials with good high-temperature performance;
③Developing new chromium-free refractory materials;
④Promoting and applying new monolithic refractory materials and high-temperature repair technologies.