1. Oxidation of carbon and formation of decarburization layer
During the use of magnesia carbon bricks, the carbon in the hot surface of the working lining will undergo oxidation reaction to form a thin decarburization layer. This oxidation process is mainly driven by two factors: one is the oxidation of carbon by iron oxides in slag and oxygen, carbon dioxide, silicon dioxide and other oxides in the air; the other is the dissolution of carbon in molten steel and the vaporization of carbon by MgO in bricks. When carbon is oxidized, a decarburization layer will be formed on the surface of magnesia carbon bricks. This layer structure is relatively weak and easily eroded by the outside.
With the formation of the decarburization layer, high-temperature liquid slag will penetrate into the pores or cracks caused by thermal stress. These slags react with magnesium oxide in the bricks to form low-melting-point compounds. These compounds not only reduce the strength of the surface layer of the bricks, but also gradually cause the surface layer to change and fall off under the action of strong stresses such as slag stirring and mechanical scouring. This process will continue to cycle, making the furnace lining gradually thinner, which may eventually lead to furnace repair, furnace repair or even shutdown.

2 The influence of pores on the damage of magnesia carbon bricks
The pores in magnesia carbon bricks, especially the open pores, have an important influence on their damage process. These pores provide channels for the oxidation of carbon, which intensifies the oxidation rate of carbon and promotes the formation of decarburization layer. In addition, the pores will inhale air from the outside when the magnesia carbon bricks are cooled, further intensifying the oxidation of carbon.
At the same time, pores are also the main way for slag to penetrate into the brick body. The slag enters the interior of the brick through the pores, reacts with magnesium oxide and other components to generate low-melting point compounds, causing the brick structure to be destroyed. In addition, pores may also cause uneven stress distribution inside the brick body, causing cracks and peeling.
In summary, the oxidation of carbon and the formation of decarburization layer and the influence of pores are the two main reasons for the damage of magnesia carbon bricks. In practical applications, corresponding measures need to be taken to address these reasons, such as optimizing the production process, improving the purity of materials, reducing the number of pores, etc., in order to extend the service life of magnesia carbon bricks and improve their performance.