During the operation of intermediate frequency furnace, the refractory material used for the lining is only 70-110mm thick. The inner side is in contact with high-temperature molten metal, while the outer side is in close contact with the water-cooled coils. The temperature difference between the inner and outer sides of the refractory material is significant, and it operates under relatively thin cross-section conditions and highly corrosive environments during many smelting operations. The main process conditions affecting lining damage include: smelting temperature, degassing time, single degassing volume, slag chemical composition, and the type of steel (iron) produced. The main factors affecting lining damage are: slag chemical corrosion, refractory material structural spalling, and thermal erosion.
01. Lining of Intermediate Frequency Furnace
The lining of intermediate frequency furnace is usually made of refractory materials of various particle sizes bonded together (commonly used refractory materials mainly include four categories: magnesia, quartz, alumina, and composite materials). Its characteristics are: direct bonding. Therefore, it has high erosion resistance, high mechanical strength, and good thermal shock resistance.
02 Damage Mechanism of Magnesia Furnace Lining Materials
Taking magnesia refractories as an example, the damage mechanism of magnesia materials is explained as follows:
The main manifestations of damage to magnesia materials are: thermal erosion caused by flowing molten steel and chemical erosion caused by the penetration of slag components into the material.
During the smelting process, the molten steel solution penetrates into the refractory matrix through the capillary channels, eroding the furnace lining. Components penetrating into the refractory matrix include: CaO, SiO2, and FeO from the slag; Fe, Si, Al, Mn, and C from the molten steel; and even metal vapor and CO gas. These penetrating components deposit in the capillary channels of the refractory material, causing a discontinuity in the physicochemical properties of the refractory working surface compared to the original refractory matrix. Under rapid temperature changes, cracks, spalling, and structural loosening will occur. Strictly speaking, this damage process is much more severe than the dissolution damage process.
The metal materials added to the furnace will bring in various oxides, and the slag composition varies depending on the material and the furnace batch. Most of the various oxides, carbides, sulfides, and complex compounds present in the slag will chemically react with the furnace lining to form new compounds with different melting points. Some low-melting-point oxides generated during the reaction, such as fir olivine (FeOSiO2) and manganese olivine (MnOSiO2), generally have melting points around 1200℃. Low-melting-point slag has excellent fluidity and may act as a flux, causing severe chemical erosion of the furnace lining and thus reducing its service life.
High-melting-point slags generated during the reaction, such as mullite (3Al2O3·2SiO2) and forsterite (2MgO·SiO2), as well as some high-melting-point metallic elements, can reach melting points above 1800℃. There is also a complex intermingling and mutual solubility between the high-melting-point and low-melting-point slags suspended in the molten metal. These slags easily adhere to the furnace wall and accumulate, causing severe slag adhesion, affecting the electric furnace’s power, melting rate, and capacity, and ultimately impacting the furnace lining’s lifespan.As furnace capacity increases, the proportion of heat lost from the molten steel surface decreases, resulting in higher slag temperatures and better slag fluidity compared to smaller capacity furnaces. This intensifies erosion of the furnace lining. Large induction furnaces often employ a mixed steel-slag tapping method, requiring slag with excellent fluidity to withstand the tapping conditions. Consequently, erosion is severe at the slag line, another reason for reduced lining lifespan. Due to these factors, the lining lifespan of large induction furnaces is shorter than that of medium and small induction furnaces. To improve lining lifespan, the lining thickness should be appropriately increased. However, as lining wall thickness increases, resistance increases, reactive power loss rises, and electrical efficiency decreases. Therefore, lining wall thickness is limited to a certain range. Thus, a reasonable wall thickness must be selected to ensure both high electrical efficiency and a sufficient lining lifespan.
03 Solution Design
The above-mentioned erosion, under cyclical temperature fluctuations, leads to so-called structural spalling. During the production process, slag penetrates into the pores of the refractory matrix, forming a large, thickened refractory layer. The physical and chemical properties of the refractory material impregnated by the slag change. Due to the difference in thermal expansion coefficients between the impregnated layer and the remaining slag layer, significant stress occurs at the interface between the two layers when the temperature changes, leading to cracks parallel to the working surface and ultimately causing the furnace lining to spall. Slag penetrating into the refractory matrix dissolves refractory particles, weakening the bond between particles, thus reducing the material’s refractoriness and high-temperature resistance. Therefore, the slag-infiltrated refractory layer deteriorates more quickly under the erosion of flowing molten steel.
The basicity of the slag should be compatible with the furnace lining material. Magnesia furnace lining materials can be eroded by high-CaO and SiO2 slags. The amount of CaF in the slag should be controlled; excessive CaF will erode the basic furnace lining, causing premature melting of the slag line zone. When the concentrations of fluoride and manganese ions in the slag are high, or when the molten pool temperature exceeds 1700℃, the viscosity of the solution decreases sharply, accelerating the damage to the furnace lining and significantly reducing its lifespan. During slag-free smelting under vacuum, the lifespan of the furnace lining is longer than that under non-vacuum smelting.
A higher iron oxide content in the furnace lining damages the original lining’s microstructure, reduces its refractoriness, and lowers the viscosity of the CaO-Al₂O₃-SiO₂ slag, allowing it to penetrate deeper into the material. However, a certain amount of iron oxide in the original lining is beneficial for rapid sintering and reducing porosity and permeability. Especially when the molding material contains a certain amount of iron oxide, the rapid sintering and prevention of sand inclusions are particularly significant.
Increasing the magnesium oxide content and slag viscosity not only reduces slag erosion of the furnace lining but also improves slag collection. When the slag basicity is low, the erosion of magnesia linings is more severe, resulting in a shorter lining life. Conversely, when the slag basicity is high, the erosion of the lining is less severe, and the lining life is relatively longer. Increasing the slag basicity and MgO content in the slag, and decreasing the FeO content, helps reduce the slag’s erosion of refractory materials. Therefore, when using slag-forming agents, it is important to select materials with high magnesium oxide content. A reasonable slag structure should be configured to accelerate slag formation, shorten smelting time, and reduce the iron oxide content in the slag.
The appropriate slag should be selected based on the lining material. Basic slag is suitable for magnesia linings but can be eroded by high-CaO and SiO2 slags. Excessive CaF2 can also erode basic linings, causing premature melting of the slag line zone. Acidic slag is suitable for quartz linings, while magnesia-alumina linings are only suitable for weakly basic or neutral slags. Alumina furnace linings exhibit typical amphoteric properties at high temperatures under varying pH levels, allowing them to adapt to slags of different pH concentrations, though slightly less so than acidic and basic furnace linings. To address this, some researchers use high-purity magnesia with the addition of spinel to modify the matrix properties of pure magnesia lining materials. However, experiments show that even high-purity corundum materials show significantly lower erosion resistance than sintered magnesia with lower purity. Acidic slags are suitable for quartz furnace linings, while magnesia-alumina linings are only suitable for weakly alkaline or neutral slags. Alumina furnace linings exhibit typical amphoteric properties at high temperatures under varying pH levels, allowing them to adapt to slags of different pH concentrations, though slightly less so than acidic and basic furnace linings.
In summary, considering the main failure mechanisms of magnesia furnace linings, through continuous summarization and exploration, the material’s resistance to slag penetration can be improved by limiting open porosity and permeability, while the high-temperature flexural strength and harsh softening temperature can be improved to enhance the high-temperature erosion resistance and spalling resistance of the lining matrix. The performance of a furnace lining depends on various factors, such as the particle size distribution of the material, its physical and chemical properties, and the sintering temperature.
04 Conclusion
1) Furnace lining materials should possess high hot strength, low permeability, and low porosity.
2) Initial damage to the furnace lining is caused by the dissolution of the sintered layer of the refractory material in the slag, resulting in frontal erosion, and by cracks appearing due to cyclic temperature changes. Another factor causing crack propagation in the overall lining is the stress generated by the different expansion coefficients between the three zones due to excessively high heating temperatures.
3) The lifespan of the furnace lining depends on proper operation, including lining inspection and timely repair of cracks using “repairing materials” to prevent molten steel and slag from seeping into the lining matrix.